Results 101 to 110 of about 5,591 (229)
Comparison of Micro Al6061-12%TiB2 with Nano Al6061-12%TiB2 Composite
Generally, attenuated actual composite materials consist of accretion like fibre, fillers and particles and are cast in a set of ceramics, metals or polymers. Owing to the backdrop of attenuated abstracts like aluminium oxide, silicon carbide, graphite etc, the composites are hardly abased.
E.S Esakkiraj +3 more
openaire +1 more source
Corrosion Characterisation of Al-Cu Reinforced In-Situ TiB2
Aluminium (Al) based in-situ metal matrix composites (MMCs) have better properties and performance compared to ex-situ MMCs. In this research, aluminium-copper (Al-Cu) alloy was reinforced with 3 and 6wt.% titanium diboride (TiB2).
Rosmamuhamadani R. +5 more
doaj +1 more source
The fully dense boron carbide matrix composites containing 10%-40% (volume fraction) TiB2(TiB2/B4C) were in-situ fabricated via chemical reaction of B4C, TiO2 and graphite powders at 2 050 degrees C under a pressure of 35 MPa.
Peng, Hua-Xin +3 more
core
Three distinct titanium diboride (TiB2) weight percentages 3%, 6%, and 9% were incorporated into Al7075-TiB2 composites by stir casting. Al7075-TiB2 composites' wear and mechanical characteristics were evaluated.
Suhas B G +3 more
doaj
Microstructure and mechanical properties of in-situ TiB2/A356 composites and a prediction model of yield strength [PDF]
The in-situ TiB2/A356 composites were successfully synthesized through the mixed salt reaction method. The advantage of this technique was that the particle sizes and morphology can be controlled by the melt reaction.
Yi-jie Zhang +2 more
doaj
Unlubricated fretting wear of TiB2-containing composites against bearing steel
Fretting tests under dry unlubricated conditions (22 degreesC to 25 degreesC, 50 to 55 pct RH) were performed on monolithic TiB2, TiB2-based cermet with a Ni-3(Al,Ti) binder, sialon-TiB2, and ZrO2-TiB2 composites to assess their relative wear performance
K. C. Hari Kumar +9 more
core +1 more source
High pressure combustion sintering of TiB2-TiC and TiB2-SiC cermic composites.
Titanium diboride based ceramic composites in the systems of TiB2-TiC and TiB2-SiC were fabricated without sintering aids by a high pressure combustion sintering process. They were synthesized and densified simultaneously from pelleted mixtures of the stoichiometric composition of Ti and B, and the powders of TiC or SiC added ( 0, 5, 10, 20, 30 wt ...
Miyamoto, Yoshinari +4 more
openaire +2 more sources
Determination of the thermodynamic stability of TiB2
The standard free energy of formation of titanium boride (TiB2) Was measured by the Electro Motive Force (EMF) method (by using yttria doped thoria (YDT) as the solid electrolyte). Two galvanic cells viz.
Pankajavalli, R +6 more
core
Microstructure-mechanical properties relations in SiC-TiB2 composite
Densification and mechanical properties (fracture toughness, flexural strength and hardness) of SiC-TiB2 composite were studied. Pressureless sintering experiments were carried out on samples containing 0-50 vol% of TiB2 created by in situ reaction ...
Krstic, Vladimir, Bučevac, Dušan
core +1 more source
C-TiB2 Composite Inert Cathode Material by Spark Plasma Sintering [PDF]
TiB2 has been considered a potential inert, wettable cathode material for aluminum reduction cells for a long time. An important characteristic of TiB2 as a cathode material, is its excellent wetting properties towards molten aluminium.
Håberg, Audun
core +1 more source