Results 81 to 90 of about 1,179,786 (407)
The fused filament‐fabricated MAR‐M247 alloy without hot isostatic pressing shows the lowest porosity of 4%. Heat treatment at 1220 °C produces coarse precipitates and carbides. Specimens heat‐treated at 1220 °C exhibit higher tensile strength (683 MPa) and elongation (10%) at room temperature.
Haneen Daoud +7 more
wiley +1 more source
Method of joining aluminum to stainless steel Patent [PDF]
Joining aluminum to stainless steel by bonding aluminum coatings onto titanium coated stainless steel and brazing aluminum to aluminum/titanium coated ...
Huschke, E. G., Jr., Nord, D. B.
core +1 more source
This work reveals the phase composition and quantitative morphology analysis of precipitation‐hardened Fe32Cu12Ni11Ti16Al29 complex‐concentrated alloy. The precipitates are shown to have a high coherency. Morphology transition between sphere, cuboidal, and elongated morphology is observed. Finally, the overaging behavior is captured using microhardness.
Rostyslav Nizinkovskyi +4 more
wiley +1 more source
Investigation of Dynamic Mechanical Behavior and Damage Characteristics in TC32 Alloy
The dynamic shearing experiment was been done by using split Hopkinson pressure bar(SHPB) technique in TC32 alloy with lamellar, bimodal and basket microstructures. The damage Characteristics of TC32 alloy was investigated by using optical microscope(OP)
LI Mingbing +6 more
doaj +1 more source
Study the effect of sliding frequency on reciprocating sliding wear test for titanium alloy Ti-6Al-4V [PDF]
Titanium alloys are widely used in the aerospace, automotive, chemical and biomedical industries. Titanium and its alloys have excellent corrosion resistance towards many of the highly corrosive environments, particularly, oxidizing and chloride ...
Ahmad Nordin, Nurani +5 more
core
In the present study, metastable CrMnNi steels with varying chemical compositions and a concomitantly altered stacking fault energy are processed via directed energy deposition and afterwards tested via tensile tests at different temperatures. The present study shows the influence of the manufacturing process on the elemental deformation mechanisms for
Julia Richter +8 more
wiley +1 more source
Porous Titanium for Biomedical Applications: Evaluation of the Conventional Powder Metallurgy Frontier and Space-Holder Technique [PDF]
Titanium and its alloys are reference materials in biomedical applications because of their desirable properties. However, one of the most important concerns in long-term prostheses is bone resorption as a result of the stress-shielding phenomena ...
Arévalo Mora, Cristina María +7 more
core +1 more source
Rotary friction welding of steel E355 and the aluminum alloy EN AW‐6082 can lead to the formation of brittle intermetallic phases. The primary process parameters are varied in order to determine their influence on this intermetallic phase formation and the resulting mechanical properties.
Laura Huber +4 more
wiley +1 more source
Ti‐6Al‐4V samples produced by laser‐powder bed fusion are tested for static and dynamic mechanical properties to systematically evaluate the effects of surface roughness and internal porosity when using productivity parameters. The most detrimental impact to fatigue is caused by surface roughness, lack of fusion and keyhole porosity in descending order.
Julian Emanuel Gunther Schulz +4 more
wiley +1 more source
Research and Development of Some Advanced High Temperature Titanium Alloys for Aero-engine
Some advanced high temperature titanium alloys are usually selected to be manufactured into blade, disc, case, blisk and bling under high temperature environment in compressor and turbine system of a new generation high thrust-mass ratio aero-engine. The
CAI Jian-ming +6 more
doaj +1 more source