Results 131 to 140 of about 510,085 (392)
The final publication is available at Springer via https://www.springer.com/gb/book/9783319956800 ; Since the turn of the 21st Century, Mental Toughness has been defined in a variety of ways (e.g. Clough, Earle & Sewell, 2002; Coulter, Mallett & Gucciardi, 2010; Fourie & Potgieter, 2001; Golby & Sheard, 2006; Gucciardi, Gordon & Dimmock, 2008; Jones ...
Strycharczyk, Doug+3 more
openaire +2 more sources
The utilization of direct energy deposition (DED)‐arc additive manufacturing processes in industrial applications is increasing, and these processes have the potential for multi‐material applications. This work provides a overview of the state of research in DED‐arc made functional graded structures, to establish a link to potential industrial ...
Kai Treutler, Volker Wesling
wiley +1 more source
Masonry structures are susceptible to damage and collapse due to seismic actions, a problem in many urban areas. To address this issue, researchers are studying the use of fibre-reinforced mortars as overlay strengthening systems. This study assessed the
João A. P. P. Almeida+2 more
doaj +1 more source
Mental toughness latent profiles in endurance athletes
Mental toughness in endurance athletes, while an important factor for success, has been scarcely studied. An online survey was used to examine eight mental toughness factors in endurance athletes.
J. Zeiger, R. Zeiger
semanticscholar +1 more source
Toughness of Confined Auxetic Foams
Auxetic (negative Poisson's ratio) materials offer benefits such as impact mitigation, thermal insulation, vibration damping, and reduced shear strain, although their fracture mechanics are largely unexplored. This study investigates damage initiation and propagation in confined re‐entrant auxetic foams from polyurethane via experimental ...
Adrianos E. F. Athanasiadis+3 more
wiley +1 more source
Tight toughness bounds for path-factor critical avoidable graphs
Given a graph G and an integer [Formula: see text], a spanning subgraph H of G is called a [Formula: see text]-factor of G if every component of H is a path with at least k vertices.
Wenqi Wang, Guowei Dai
doaj +1 more source
Influence of heat treatment on mechanical properties of steel
This article concerns an influence of heat treatment on strength and toughness of steel. The partial results of tests on steel 12 042 are presented.
R. Chotěborský, M. Brožek
doaj +1 more source
Effect of Li level, artificial aging, and TiB2 reinforcement on the fracture toughness of Weldalite (tm) 049-type alloys [PDF]
Plane strain fracture toughness (K sub IC) was evaluated for Weldalite (tm) 049 with and without TiB2 reinforcement. For the nonreinforced variant, changes in toughness were measured for various aging conditions and lithium levels.
core +1 more source
Fracture toughness and crack-resistance curve behavior in metallic glass-matrix composites [PDF]
Nonlinear-elastic fracture mechanics methods are used to assess the fracture toughness of bulk metallic glass (BMG) composites; results are compared with similar measurements for other monolithic and composite BMG alloys.
Hofmann, D. C.+5 more
core +2 more sources
Direct Natural and Artificial Aging of Aluminum Alloy AlSi10Mg After Laser Powder‐Bed Fusion
Laser powder‐bed fusion of metals aluminum alloy AlSi10Mg has been directly aged. Artificial aging after natural aging is considered. The hardening potential is high for the top part of the samples as well as after short natural aging. The hardening potential is substantially reduced for the bottom part of the samples, as well as after natural aging of
Rabea Steuer+6 more
wiley +1 more source