Results 211 to 220 of about 4,796,670 (284)
Influence of Ferrule Height and Uniformity on Fracture Resistance of Post-core Crowns: An In Vitro Analysis. [PDF]
Rk M, Vilas V, Gowda A.
europepmc +1 more source
Zein‐Based Adhesives: Sustainable Extraction and Application in Bioadhesive Technologies
Zein is extracted from corn gluten meal using a simple and scalable process with high yield (~90%). The resulting protein is applied in bioadhesives modified with Ca2+ and Fe3+ ions, exhibiting substrate‐dependent adhesion. The findings demonstrate competitive bonding performance and highlight the role of ionic interactions in tuning adhesion ...
Paula Bertolino Sanvezzo +3 more
wiley +1 more source
The thermal diffusivity of MgO‐C refractories is highly sensitive to sample preparation and processing procedures. In this article, the effects of coking sequence, machining conditions, structural inhomogeneity, and graphite coating application on measurements using laser flash apparatus are systematically investigated.
Luyao Pan +4 more
wiley +1 more source
It is shown that laser ablation pretreatment under oxygen‐free conditions enables copper–aluminium bonding at significantly lower deformation degrees and improved properties compared to mechanical brushing. Laser ablation further increases interface contact area and induces favourable residual stress states and microstructural compatibility ...
Khemais Barienti +11 more
wiley +1 more source
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
Microdroplet Templating of Uniform Nanostructured Battery Microparticles with Scalable Membrane Emulsification. [PDF]
Sanders KA +4 more
europepmc +1 more source
Stabilization of L‐PBF Ni50.7Ti49.3 under low‐cycle loading was investigated. Recoverable strain after cycling was dependent on the amount of applied load. Recovery ratio was 53.4% and 35.1% at intermediate and high load, respectively. The maximum total strain reached 10.3% at a high load of 1200 MPa.
Ondřej Červinek +5 more
wiley +1 more source
Creep experiments at 900°C on coarse‐grained steel‐ceramic composites containing recycled magnesia reveal that higher ceramic volume fractions significantly enhance the creep resistance. Detailed EBSD investigations identify subgrain formation in the steel matrix as the dominant deformation mechanism.
Moritz Müller +6 more
wiley +1 more source
Noise-induced instability of uniform flow in single-file traffic systems. [PDF]
Dufour O +5 more
europepmc +1 more source