External and Internal Cracking Caused by Heat Treatment in Laser Powder Bed Fusion‐Fabricated Inconel 738LC Components

open access: yesAdvanced Engineering Materials, EarlyView.
Manufacturing problems such as heat treatment‐induced cracking hinder the widespread application of the laser powder bed fusion (LPBF) process to superalloys. In this study, cracks in the LPBF components of Inconel 738LC superalloy are characterized after heat treatment at various temperature ranges, revealing two distinct cracking behaviors.
Kosuke Kuwabara   +4 more
wiley   +1 more source

Additive Manufacturing of Alumina‐Reinforced Elastomers

open access: yesAdvanced Engineering Materials, EarlyView.
Vat‐photopolymerized elastomers reinforced with platelet‐shaped alumina exhibited preferential orientation, reduced porosity, and significantly enhanced mechanical performance. A 3 wt% platelet loading increased tensile strength from 12.4 to 45.7 MPa, highlighting the critical role of filler morphology in elastomeric VPP composites.
Majid Barzegar Keyvani   +6 more
wiley   +1 more source

DigiChrom: A Domain Ontology for Semantic Representation of Trivalent Chromium Platings and Its Large Language Model‐Based Alignment With Multiple Mid‐Level Ontologies

open access: yesAdvanced Engineering Materials, EarlyView.
Digitalizing electroplating requires both domain knowledge and interoperability. This work introduces PlatOn, a domain ontology for trivalent chromium plating and coating characterization, and a hybrid pipeline that aligns it to a mid‐level reference ontology by combining eight similarity metrics with language model reasoning. Expert‐validated mappings
Janik Harter   +10 more
wiley   +1 more source

On the Effect of Creep on Local Lattice Orientation in Single‐Crystal Ni‐Based Superalloy Microstructures

open access: yesAdvanced Engineering Materials, EarlyView.
During creep of a single‐crystal Ni‐based superalloy, the overall crystal orientation is observed to remain constant while the microstructure evolves. Despite the lack of macroscopic rotation, small (<1°) rotations are observed on the submicron size scale and are accommodated by counteracting rotations over the scale of several micrometers.
E. J. Payton   +3 more
wiley   +1 more source

Distinct Microstructural Characteristic Lengths Defining Notch Fatigue Crack Initiation and Propagation, and Defect Tolerance in Advanced Steels

open access: yesAdvanced Engineering Materials, EarlyView.
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...