Historical Foundation and Practical Guideline for Ferroelectric Switching Kinetic Studies
The P and U pulses in the conventional PUND measurements are not identical because of the interplay between switching current and the measurement circuit components. This circuit effect can lead to a shift in polarization transients and misinterpreted physics in the switching kinetics.
Yi Liang, Pat Kezer, John T. Heron
wiley +1 more source
We use scanning nitrogen vacancy magnetometry to directly image the weak in‐plane magnetic moments in mixed phase BiFeO3 at the nanoscale and quantify the local magnetic moments to be 18.8±2.0 μB/nm2 in the rhombohedral‐like phase and 1.5±0.6 μB/nm2 in the well‐known non‐magnetic tetragonal‐like phase.
Lei Wang +14 more
wiley +1 more source
Glissile Interphase Boundaries Enable Collective Phase Switching in Epitaxial Polar Oxides
A triple point is identified in the phase diagram of low‐symmetry epitaxial BiFeO3 thin film along with an extended regime of phase competition associated with a flattened energy landscape. The electromechanical response is shown to be governed by correlated interphase‐boundary motion, including scale‐free avalanche dynamics characteristic of systems ...
Mohammad Moein Seyfouri +11 more
wiley +1 more source
Advances in Sustainable and Wearable Textile Based Soft Robotics
This Review examines advances in wearable textile‐based soft robotics, focusing on sustainable materials, integrated sensing, and scalable actuation. It discusses manufacturing and system integration across healthcare, assistive robotics, prosthetics, and human–machine interfaces, and highlights key challenges in circular design, including life‐cycle ...
Zahir Abbas +6 more
wiley +1 more source
Notice re renaming of Sea Level Datum 1929 to National Geodetic Vertical Datum of 1929
National Vertical Control Net
core
Structure‐Guided Dynamical Mechanics in Bioinspired Double Twisted Laminated Thin Films
This work explores a dynamic mechanistic study of crack propagation and puncture testing via real‐time monitoring of crack initiation, propagation, and termination through nature‐inspired single and double twisted architectures fabricated from cellulose nanocrystals.
Justin Brackenridge +4 more
wiley +1 more source
A giant magnetic coercivity and a vertical shift of hysteresis loops are demonstrated in Sr3YCo4O10+δ epitaxial films. The hard magnetic behavior originates from ferromagnetic spin bags stabilized within a long‐range ordered oxygen‐vacancy structure.
Yanbin Chen +12 more
wiley +1 more source
Ferroelectric nanoclusters create local internal fields in a normally non‐switchable polar film because of polarization mismatch at their interfaces. That field opposes polarization in the regions with larger polarization and reinforces polarization in the regions with smaller polarization.
Anna N. Morozovska +5 more
wiley +1 more source
Monolithic UV‐ozone oxidation of Ta forms an ultrathin Ta2O5/TaOx bilayer enabling resistive switching with a vertical defect gradient. A stoichiometric surface layer over an oxygen‐deficient sublayer promotes localized filament nucleation near the top interface, enabling low‐voltage operation, and reduced cycle‐to‐cycle variability.
Seunghoon Yang +11 more
wiley +1 more source