Results 61 to 70 of about 111,237 (217)

Effects of aluminum oxide addition on the flexural strength, surface hardness, and roughness of heat-polymerized acrylic resin

open access: yesJournal of Dental Sciences, 2012
Background/purpose: Acrylic dentures frequently fracture during service due to their poor strength characteristics. The aim of this study was to evaluate the effects of adding 0.5–5 wt% aluminum oxide (Al2O3) powder on the flexural strength, surface ...
Mahroo Vojdani   +2 more
doaj   +1 more source

Dynamic drilling as an alternative method for determining the mechanical behavior of refractories materials

open access: yesTecnoLógicas, 2017
Ceramic materials hardness is usually determined by Vickers microindentation, which requires rigorous sample preparation and highly demanding analysis of traces turning this method difficult to use in industrial applications.
Daniel Zuluaga-Castrillón   +4 more
doaj  

Mechanical Behavior Analysis of a Friction Stir Welding (FSW) for Welded Joint Applied to Polymer Materials

open access: yesFracture and Structural Integrity, 2018
Welding is a technique of fusion joining the material involving a process of inter-molecular diffusion adhesion. Polymer welding is an assembly method among several known assembly techniques such as gluing. This welding process applies to thermoplastics;
Hachellaf kaddour   +3 more
doaj  

Mechanical Properties of Ni-Cr-Al Alloy Cold Drawn Bar [PDF]

open access: yesTeshugang
In this paper, the preparation of Ni-Cr-Al alloy by the smelting process of 200 kg vacuum induction + vacuum arc remelting(VIM+VAR) was analyzed by means of tensile test at room temperature, optical microscope and hardness test (/%:0.01C, 0.10-0.20Si, 0 ...
Liu Junkai, Yu Yipeng, Shen Yaqiu, Wang Jing, Luo Xi, Zhang Jiansheng
doaj   +1 more source

Comparison of Plasma Transferred Arc and Submerged Arc Welded Abrasive Wear Resistant Composite Hardfacings

open access: yesMedžiagotyra, 2018
EComposite hardfacings produced by Plasma Transferred Arc Welding (PTAW) and Submerged Arc Welding (SAW) possess a good combination of hardness, wear resistance and fracture toughness, thus providing high wear resistance.
Taavi SIMSON   +5 more
doaj   +1 more source

Microstructure Characterisation, Hardness, and Corrosion Behaviour of Nickel-Silicon Carbide Electrodeposition Coating with The Influence of Ultrasonic Agitation [PDF]

open access: yesArchives of Metallurgy and Materials
This study is about the electrodeposition of Ni-SiC composite coatings at various ultrasonic agitation temperatures (50, 55, and 60°C). The coatings were characterised by a scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS ...
A. Loganathan   +5 more
doaj   +1 more source

The effect of different types of oral mouth rinses on the hardness of Silorane-based and Nano-hybrid composites

open access: yesSaudi Journal of Oral Sciences, 2014
Background: The restorative materials used in dentistry are required to have long-term durability in the oral cavity. Effect of various fluids in the oral environment can affect the hardness of these restorations.
Rohit Ashok Antony Fernandez   +3 more
doaj   +1 more source

Indentation Size Effect on the Hardness of Silicon Carbide Ceramics [PDF]

open access: yesKemija u Industriji, 2010
The Vickers hardness of CVD SiC ceramics is determined as a function of the indentation load. Vickers hardness pyramid-shaped sharp diamond indenter with angle between opposite faces at an angle of 136° was used to apply five indentation loads of 4.91; 9.
.Grilec, K:, Rede, V., Ćurković, L.
doaj  

The Impact of Damage in Inconel 718 on Hardness Measured by the Vickers Method

open access: yesFatigue of Aircraft Structures, 2015