Zein‐Based Adhesives: Sustainable Extraction and Application in Bioadhesive Technologies

open access: yesAdvanced Engineering Materials, EarlyView.
Zein is extracted from corn gluten meal using a simple and scalable process with high yield (~90%). The resulting protein is applied in bioadhesives modified with Ca2+ and Fe3+ ions, exhibiting substrate‐dependent adhesion. The findings demonstrate competitive bonding performance and highlight the role of ionic interactions in tuning adhesion ...
Paula Bertolino Sanvezzo   +3 more
wiley   +1 more source

Investigation of Laser Ablation and Brush Pre‐Treatments for AlCu Cold Roll Bonding in Oxygen‐Free Conditions

open access: yesAdvanced Engineering Materials, EarlyView.
It is shown that laser ablation pretreatment under oxygen‐free conditions enables copper–aluminium bonding at significantly lower deformation degrees and improved properties compared to mechanical brushing. Laser ablation further increases interface contact area and induces favourable residual stress states and microstructural compatibility ...
Khemais Barienti   +11 more
wiley   +1 more source

Microstructural Evolution and Vacancy Defect Formation in Mn–Mo–Ni RPV Steel Under Low Cycle Fatigue: Insights From EBSD and PALS

open access: yesAdvanced Engineering Materials, EarlyView.
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar   +2 more
wiley   +1 more source

EBSD Study of Creep‐Induced Lattice Misorientation in MgO‐Particle‐Reinforced Austenitic Steel Composites

open access: yesAdvanced Engineering Materials, EarlyView.
Creep experiments at 900°C on coarse‐grained steel‐ceramic composites containing recycled magnesia reveal that higher ceramic volume fractions significantly enhance the creep resistance. Detailed EBSD investigations identify subgrain formation in the steel matrix as the dominant deformation mechanism.
Moritz Müller   +6 more
wiley   +1 more source

Reduction of Oxide Inclusions During the High‐Frequency Welding of Steel via a Nonthermal Ar/H2 Plasma Jet

open access: yesAdvanced Engineering Materials, EarlyView.
High‐frequency (HF) welding of steel is limited by oxide inclusions that degrade weld quality. This study demonstrates, for the first time, the integration of a nonthermal Ar/H2 dielectric barrier discharge (DBD) plasma jet into HF welding. Local plasma treatment provides effective shielding and in‐situ oxide reduction, resulting in markedly fewer and ...