Results 41 to 50 of about 2,919 (265)
As a new type of high-efficiency welding process, the magnetically controlled double-wire single-arc MAG welding has poor arc controllability and is easily affected by external interference during the welding process.
Qian ZHANG +4 more
doaj +1 more source
Weld quality is generally determined by reinforcement and penetration depth of weld bead in arc welding. Penetration depth reflects weld strength and reinforcement reflects weld shape. What's more, there is a strong coupling between them, therefore it is
Jun Lu +4 more
doaj +1 more source
Without adding any interlayers or coatings, the lap welding experiment of AZ31B magnesium alloy and DP980 high-strength steel was performed with the laser-induced tungsten inert gas welding (TIG) arc technology. Through optimizing the process parameters,
SONG Gang +3 more
doaj +1 more source
Thermomechanical fatigue tests of laser beam powder bed fusion (PBF‐LB) Inconel 718 show that the additively manufactured material reaches almost the lifetimes of conventionally‐rolled material under no‐dwell conditions. Introducing dwell times at the maximum temperature markedly reduces the lifetimes due to pronounced grain boundary sliding associated
Stefan Guth +6 more
wiley +1 more source
Double-wire arc welding involves simultaneously feeding two wires into a molten pool, improving the efficiency and flexibility of traditional welding techniques.
Bolun Dong +4 more
doaj +1 more source
Influence of an Oxygen‐Free Atmosphere on Diamond‐Single‐Grain Scratching of Ti–6Al–4V
Single‐grain scratching of Ti–6Al–4V is investigated under controlled, oxygen‐free, and ambient atmospheres using a novel experimental setup with in situ high‐speed imaging. The approach enables direct observation of chip formation and adhesion under suppressed oxidation.
Berend Denkena +2 more
wiley +1 more source
Clockwise circular oscillation (CW) laser welding experiments are carried out on 8.0 mm thick 5A06 aluminum alloy. Considering the beam oscillating trajectory and energy superposition effect, the energy distribution model of the workpiece surface is ...
Jiasi CAI +4 more
doaj +1 more source
The formation of nonmetallic inclusions (NMIs) was investigated in this study, carrying out immersion tests for 30 min at a temperature of 1600°C with liquid high‐silicon electrical steel (Si ≈ 3 mass‐%) and different MgO–C refractories. Conventional MgO–C refractories were considered, as well as MgO–C refractories containing MgO–C recyclate and ...
Lukas Neubert +6 more
wiley +1 more source
This study investigates laser‐based oxide removal of Cu inserts in oxygen‐free conditions and examines long‐term oxidation kinetics and surface chemistry under different atmospheres via X‐ray photoelectron spectroscopy. Al–Cu compound casting with differently oxidized surfaces is performed, and intermetallic phase formation, morphology, and thermal ...
Timon Steinhoff +9 more
wiley +1 more source
On the Determination of the Forming Limits of Low-Alloy Steel Thin-Walled Tubes [PDF]
This paper presents an innovative methodology to determine the formability limits of low-alloy steel tubes, with particular attention to the effects of the weld line on their performance.
Magrinho João +4 more
doaj +1 more source