Pattern Recognition of Pipeline Magnetic Memory Inspection Based on BP Neural Network
To distinguish the magnetic memory signals of different damage forms at the base material of the pipeline and the weld joint, the BP neural network is used to identify the pattern of the pipeline defect inspection signal.
Shi Xiaodong +4 more
doaj
Effect of Butt Gap on Stress Distribution and Carrying Capacity of X80 Pipeline Girth Weld. [PDF]
Zhu L, Jia H, Li X, Luo J, Li L, Bai D.
europepmc +1 more source
Mechanical property degradation of X80 pipeline steel due to microbiologically influenced corrosion caused by Desulfovibrio vulgaris. [PDF]
Li Z +7 more
europepmc +1 more source
Effect of H2S Corrosion on the Fracture Toughness of the X80 Pipeline Steel Welded Joint. [PDF]
Wang X, Wang D, Deng C, Li C.
europepmc +1 more source
Formation and evolution of inclusions in the refining process of X80 pipeline steel
To further meet the requirements for using pipeline steel in extreme environments and to improve its safety in service, the inclusion control level in pipeline steel urgently needs improvement. In this paper, the variation laws of inclusion type, size, and composition in the refining process of X80 pipeline steel were studied through industrial trial ...
Hua-jun ZHONG +5 more
openaire +1 more source
The thermal cycles associated to friction stir welding and processing produce a wide range of microstructures, resulting in different mechanical behaviors along the weld.
Rodriguez, Johnnatan +16 more
core +1 more source
Effect of Post-Weld Heat Treatment on Microstructure and Fracture Toughness of X80 Pipeline Steel Welded Joint. [PDF]
Wang X +6 more
europepmc +1 more source
Statistical Assessment of Fracture Toughness Results from the HAZ of X80 Pipeline FCAW Girth Weld. [PDF]
Chen H +5 more
europepmc +1 more source
Experimental Investigation on Corrosion Behavior of X80 Pipeline Steel under Carbon Dioxide Aqueous Conditions. [PDF]
Chen J, Wang X, Ma H, Huo Z, Wang Y.
europepmc +1 more source
Corrosion behavior of X80 pipeline steel local defect pits under static liquid film. [PDF]
Tan Z +6 more
europepmc +1 more source