Results 21 to 30 of about 538 (176)
Herein, a new method is developed by combining scanning Kelvin probe force microscopy measurements with finite‐element modeling, studying the hydrogen atom diffusion and distribution in ferrite and bainite phases contained in X80 pipeline steel. The hydrogen atom concentrations in lattice and trap sites in the two phases are determined.
Qing Hu, Yufeng Frank Cheng
wiley +1 more source
Precipitates in Nb and Nb–V Microalloyed X80 Pipeline Steel [PDF]
AbstractPrecipitates in two X80 pipeline steels were studied by transmission electron microscopy equipped with an energy filtering system. The steels are microalloyed with niobium and niobium–vanadium (Nb–V), respectively, and produced by continuous hot rolling.
Zhongyi, Li +3 more
openaire +2 more sources
A new analytic method for the buried pipeline crossing the normal fault based on the shape function. Abstract Oil and gas pipelines that go through an active normal fault often deform largely and cause serious disasters. On the basis of the beam theory of the elastic foundation and assuming a shape function for the deformed pipeline, a new analytical ...
Wen‐jun Hu +4 more
wiley +1 more source
The corrosion behavior of X80 pipeline steel in 3.5 wt.% NaCl solution and simulated Dagang soil solution under different alternating current (AC) electrical densities was studied using the weight loss method, and was tested and analyzed using the ...
Xinhua Wang +3 more
doaj +1 more source
Research on Material Selection Method and Brittle Fracture Mechanism of High‐Pressure Pipeline
Aiming at the problem of the brittle fracture of pressure pipeline, the elastic constraint structure is described by using members and engineering building structures, and the concept of elastic constraint is proposed. Through the stress field analysis of the pressure pipeline under internal pressure, it is found that the pressure pipeline under ...
Yulin Li, Zhihui Li, Guangjian Dong
wiley +1 more source
China-Russia Eastern Gas Pipeline is characterized by ultra-large diameter, high grade steel (X80) and high pressure rating. It is located in the area with geologically active permafrost and semi-permafrost zones in the north, where is prone to ...
Yukun LI +4 more
doaj +1 more source
The effect of hydrogen on the fracture toughness of friction‐stir welded API 5L X70 pipeline steels
Abstract The hydrogen embrittlement (HE) leads to severe steel degradation of mechanical properties. The hydrogen atoms diffuse into the steel and get positioned into reversible and irreversible trap sites. The pipe to transport oil and gas needs to be welded to construct long‐distance pipeline projects; thus, friction‐stir welding (FSW) has proven an ...
Joseane M. Giarola +5 more
wiley +1 more source
Characterisation of the crack tip plastic zone in fatigue via synchrotron X‐ray diffraction
Abstract This paper describes a new methodology for characterising the plastic zone ahead of a fatigue crack. This methodology is applied to a set of experimental data obtained by synchrotron X‐ray diffraction on a bainitic steel compact tension specimen.
Manuel Carrera +6 more
wiley +1 more source
Influence of operation condition on in-service welding temperature field of X80 natural gas pipeline
In order to study the influence law of natural gas transportation parameters on temperature field in the heat affected zone of in-service welding in X80 natural gas pipeline, the X80 natural gas pipeline with a diameter of 1 422 mm and a wall thickness ...
Wangyou ZHU
doaj +1 more source
Abstract Corrosion of iron‐containing metals under sulfate‐reducing conditions is an economically important problem. Microbial strains now known as Desulfovibrio vulgaris served as the model microbes in many of the foundational studies that developed existing models for the corrosion of iron‐containing metals under sulfate‐reducing conditions. Proposed
Toshiyuki Ueki, Derek R. Lovley
wiley +1 more source