Simulation of Natural Gas Pipeline Networks Based on Roughness Optimization Algorithm and Global Mesh Refinement

open access: yesEnergy Science &Engineering, Volume 13, Issue 4, Page 1567-1576, April 2025.
A new numerical simulation method is developed for natural gas pipeline systems based on roughness optimization and global mesh refinement, coupled with the measured data of SCADA system. The accuracy of the proposed method is verified by the actual pipeline examples.
Yi Yang
wiley   +1 more source

Research of ultra-fine bainite X80 pipeline plate for gas compressor station

open access: yesMATEC Web of Conferences, 2018
This paper reports on the research of low temperature (-51°C) X80 pipeline plate used for gas compressor station. In order to satisfy the performance requirements of low temperature X80 pipeline plate, an optimized rolling and cooling process was ...
Li Shaopo, Ding Wenhua, Zhang Hai
doaj   +1 more source

Classification of pitting corrosion damage in process facilities using supervised machine learning

open access: yesThe Canadian Journal of Chemical Engineering, Volume 103, Issue 1, Page 153-169, January 2025.
Abstract Corrosion is widely known to be a major cause of the failures in process facilities. Prediction of corrosion damage is therefore essential for industries to manage the availability of their assets. This research aims to investigate the application of supervised machine learning methods for the classification of pitting corrosion damage ...
Parth Patel   +5 more
wiley   +1 more source

Effect of Base Metal Microstructure on Softening Behavior of the Heat-Affected Zone of X80 GMAW Girth Weld

open access: yesMetals
Softening in the heat-affected zone (HAZ) of high-strength pipeline welds compromises its service safety but the corresponding softening mechanism is not well-understood.
Xueda Li   +5 more
doaj   +1 more source

Strain capacity analysis of the mismatched welding joint with misalignments of D 1,422 mm X80 steel pipelines: An experimental and numerical investigation

open access: yesJournal of Pipeline Science and Engineering, 2021
Anomalies as misalignment, microcrack are inevitable for large diameter high strength steel pipelines. To ensure the strain capacity of mismatched welding joint with misalignments of D 1,422 mm X80 steel pipeline, a comprehensive study via wide plate ...
Yue Yang   +6 more
doaj   +1 more source

Experimental Study on Quick‐Locking Reinforcement Model for Local Defects in Pipelines in the Rich Water Area

open access: yesEngineering Reports, Volume 7, Issue 1, January 2025.
The study reveals high‐pressure buckling in quick‐lock sleeves and proposes a reliable design model. These research findings offer valuable guidance for the structural design and construction of localized repairs in municipal water supply and drainage networks.
Zhicheng Luo, Xuefeng Yan
wiley   +1 more source

Effect of Microstructural Constituents on Hydrogen Embrittlement Resistance of API X60, X70, and X80 Pipeline Steels [PDF]

open access: yesArchives of Metallurgy and Materials
This study describes how microstructural constituents affected the hydrogen embrittlement resistance of high-strength pipeline steels. The American Petroleum Institute (API) X60, X70, and X80 pipeline steels demonstrated complicated microstructure ...
Seung-Hyeok Shin   +3 more
doaj   +3 more sources

Preliminary Evaluation of the Influence of Hydrogen on the Fracture Toughness of an X65 Gas‐Transmission Pipeline Steel

open access: yesAdvanced Engineering Materials, Volume 26, Issue 16, August 2024.
We measured two values of fracture toughness for X65 steel in air (KQ of 369 and 487 MPa√m$\sqrt{} \text{m}$) and two essentially American Society for Testing of Materials–valid values of fracture toughness of KJ1C of 150 and 189 MPa√m$\sqrt{} \text{m}$ for X65 subjected to in situ hydrogen charging thought to be equivalent to a hydrogen gas pressure ...
Md Fahdul Wahab Chowdhury   +11 more
wiley   +1 more source

Full‐scale testing of near‐neutral pH stress corrosion cracking growth behavior of a vintage X52 oil pipe

open access: yesFatigue &Fracture of Engineering Materials &Structures, Volume 47, Issue 5, Page 1638-1655, May 2024.
Abstract This study presents an experimental investigation conducted on a 40‐year‐old vintage X52 oil pipe segment to assess the growth behavior of near‐neutral pH stress corrosion cracking (SCC). Six cracks were introduced on the pipe specimen, each of which was associated with a unique combination of metallurgical and environmental condition.
Haotian Sun   +5 more
wiley   +1 more source

Corrosion behavior of X80 pipeline steel in a simulated soil solution at different temperatures

open access: yesInternational Journal of Electrochemical Science
For the X80 pipeline steel, electrochemical impedance spectroscopy and potentiodynamic polarization curves were employed to examine the electrochemical corrosion behaviors of its base metal and weld joint under varying test in NS4 simulated soil solution.