Results 61 to 70 of about 806,157 (210)
Strain model and experimental study of elastic viscoplastic for crack-tip zone of X80 steel pipe
The mechanical state of the process zone at the crack-tip is one of the main factors that affect crack initiation and growth in the long-term safe operation of oil and gas pipelines. Many tests showed that the stress and strain fields in the fracture-tip
Shaohua Dong +7 more
doaj +1 more source
Abstract Microbiologically influenced corrosion (MIC) is acknowledged as a significant type of corrosion due to its extensive impact on metal/alloy surfaces. As MIC accounts for 20% of all corrosion instances, it is a critical factor causing service failure of engineering materials such as steel and aluminium alloy.
Brinda +4 more
wiley +1 more source
Quenching Temperature‘s Impact on the Microstructure and Mechanical Properties of X80 Pipeline Steel
The state study on mechanical properties’ changes of X80 steel at different quenching temperature. The results showed that the quenching temperature is 1000 °C, X80 Austenite grain coarsening is serious, leading to the production of coarse lath bainite ...
Yong Jie Ma +2 more
core +1 more source
Effect of Nb Content and Second Heat Cycle Peak Temperatures on Toughness of X80 Pipeline Steel
The microstructure evolution and variation of impact toughness in the heat-affected zone (HAZ) of X80 pipeline steel with different Nb content under different peak temperatures in the secondary thermal cycle were studied through welding thermal ...
Yaobin Yang +6 more
core +1 more source
Hydrogen Embrittlement Sensitivity of X80 Pipeline Steel Welded Joints in Hydrogen Environment [PDF]
In order to explore the changes in fracture mechanical properties of pipeline steel welded joints in hydrogen environment, the notched tensile in-situ hydrogen charging method was used to study the hydrogen embrittlement susceptibility of X80 steel base ...
LI Tianlei, LI Ke, SHI Daiyan, FENG Min, YANG Zhiwen, CHEN Yingfeng, WANG Xiuyun, LIN Yuanhua, YU Zifeng
doaj +1 more source
Austenite decomposition in an X80 linepipe steel
The final microstructure and resulting mechanical properties in the heat-affected zone (HAZ) of welded linepipes are predominantly determined by austenite decomposition during cooling after welding processes. Thus, a full understanding of continuous cooling transformation of austenite is a key step toward improving the overall performance of linepipes.
openaire +1 more source
A new numerical simulation method is developed for natural gas pipeline systems based on roughness optimization and global mesh refinement, coupled with the measured data of SCADA system. The accuracy of the proposed method is verified by the actual pipeline examples.
Yi Yang
wiley +1 more source
Corrosion effect of Bacillus cereus on X80 pipeline steel in a Beijing soil environment
The corrosion of X80 pipeline steel in the presence of Bacillus cereus (B. cereus) was studied through electrochemical and surface analyses and live/dead staining.
Song, Dongdong +7 more
core +1 more source
An investigation into the electrochemical corrosion behavior of X80 pipeline steel under different elastic and plastic tensile stress in a CO2-saturated NaCl solution has been carried out by using open-circuit potential, potentiodynamic polarization ...
Wei Wu +5 more
doaj +1 more source
The stress corrosion cracking (SCC) behavior of X80 pipeline steel under Desulfovibrio desulfurican (D. desulfurican), alternating current (AC) and cathodic protection (CP) was studied by the constant load tests and slow strain rate tensile (SSRT) test ...
Qi Fu +5 more
doaj +1 more source