Results 1 to 10 of about 699,756 (63)
Practice of Control for [Ti] Melting Loss during Stainless Steel 1Cr18Ni9Ti 1.2 t Ingot ESR Process
The effect of Ti content in steel lCrl8Ni9Ti electrode- [Ti] (0. 586% ~0. 839% ) , TiO2content in slag- (TiO2) (2. 1% ~4. 8% ) and packed ratio (0. 2 ~0. 4) (area of electrode / area of mold) on average melting loss of [Ti] during 1.
何润, 周立新, 胡长伟, 张洲
doaj
The electroslag-remelting (ESR) test on steel Cr13Mn4Mo by 70CaF2-30Al2O3slag series has been carried out. The total oxygen content, sulfur content and amount, size and morphology of inclusions in Ф55mm electrode and Ф120mm (36kg) ESR ingot are analyzed ...
张钊 +5 more
doaj
The effect of argon flow rate (15~45 L/min) , triple slag (/% : 63CaF227Al2O310CaO), quaternary slag (/% : 53CaF222Al2O320CaO, 5MgO) and pentary slag (/%: 50CaF222Al2O320CaO, 5MgO, 3TiO2) , and adding Al powder in ESR process on [Ti] in 3 t shielding ...
王海江, 徐朋, 杨松
doaj
Based on strong crack sensitivity and requiring high cleanliness of TWIP steel, with analysis and calculation the 14 t TWIP steel ESR ingot (/%: 0. 03C, 2. 88Si, 24. 71 Mn, 0. 021P, 0. 007S, 2.
郭军儒 +5 more
doaj
Optimization of Process for Hollow Forgings of ESR Alloy Steels
Typical hollow forgings-electro-slag remelting (ESR)alloy steel roll sleeve with inner diameter 560~880 mm, outer diameter 670~1200 mm and length 1300~1780 mm is usually produced by ≥2 t ingots.
赵新, 刘德富
doaj
The statistics and regression analysis on the effect of diameter of ESR ingot (Φ250 mm ~ Φ400 mm) and reduction ratio (11. 10 ~92.46) of high speed steel M2 (/% : 0.85 - 0.90C, 5.8 - 6.2W, 4.
邵青立, 谢志彬, 张国平
doaj
The electrode of René88DT nickel allov ( % : 0.02 ~ 0.05C. 15.5 ~ 16.5Cr, 3.8 ~4.2Mo, ≤0.20Ta, 12.5 ~13.5Co,0.6~1.0Nb, 0.025 ~0.050Zr, 3.5~3.9Ti, 2.0〜2.4AI, 0.006〜0.015B, 3.8〜4.2W, 0.005 ~ 0.010Ce) is melted by a 200 kg vacuum induction furnace and the ...
陈希春, 付锐, 冯涤, 任昊
doaj
The effect of adding La alloying methods on yield of La in stainless steel Fe-20Cr-5Al (/%: 0. 004 ~ 0. 006C, 0. 18Si, 0. 08Mn, 20.25 ~ 20. 28Cr, 5. 06 ~5.
余晓艳 +4 more
doaj
提出一种利用电容测量生物质灰渣熔融状态的方法,以低熔点的玉米芯灰为样品进行测试,并与X射线荧光分析(XRF)、X射线衍射分析(XRD)、热重-差热分析(TG-DSC)结果进行比较.实验结果表明:玉米芯灰样在600-1000℃加热过程中质量的减少主要由灰分中KCl随加热过程挥发所致,并影响灰熔融温度预测结果;灰样烧结温度为800-900℃,电容测试结果为825℃,TG-DSC测试结果为875℃,灰熔点仪测试结果为990℃.电容测量结果与灰样熔融结渣情况一致,电容变化可准确反映灰样相变情况 ...
周肇秋 +5 more
core +4 more sources
Improvement of 2 t GH2132 Alloy ESR Ingot Remelting Process
The GH2132 alloy (1.90% ~2. 30%Ti) has the problems of large loss of Ti element ( A[Ti]0. 37% ~ 0. 57% ) in ESR process, the Ti content in steel is only 1. 83% ~ 1. 89% in ESR middle and last period.
崔利民 +3 more
doaj