Results 31 to 40 of about 160,422 (158)
ABSTRACT The inherent brittleness of hardmetals stems from the rigid covalent bond in the ceramic matrix and the sharp ceramic/metal interface, which restricts the nucleation and motion of dislocations. In this study, a novel strategy is proposed to activate significant dislocation behaviors in the WC matrix by employing a non‐equiatomic CoNiFeCr ...
Cheng Qian +9 more
wiley +1 more source
Abstract Chinese consumer demand for ivory threatens vulnerable African elephant populations, despite long‐standing efforts to combat the illegal wildlife trade. Behavioural science approaches have been proposed to address these systemic behaviours. However, their robust use remains uncommon in demand management interventions.
Molly R. C. Brown +3 more
wiley +1 more source
为了深入揭示复合绝缘子脆断机理并提出预防措施,分析了一起500 kV复合绝缘子脆断事故,采集故障绝缘子与正常绝缘子样本进行对比试验。对样本绝缘子进行外观检查、解剖测试、拉力和耐应力腐蚀测试、憎水性测试等试验,并对试验结果进行实验室条件下的分析。结果表明:故障复合绝缘子存在3层较为明显的光滑断面,且断面处芯棒与硅橡胶护套交界面处存在硅橡胶粉化层;6只试验绝缘子只有2只通过耐应力腐蚀试验;试验绝缘子憎水性等级在HC4~HC5之间;元素分析发现脆断绝缘子芯棒中硼元素含量较高,结合测试结果可知芯棒为非耐酸芯棒 ...
卢明 +5 more
doaj
ABSTRACT Nb‐Si‐based superalloys are considered as the most potential candidate materials for nickel‐based superalloys due to the lower density and higher using temperature. Here, a type of stable Nbss/γNb5Si3 bi‐phases structure with a coherent interface has been successfully designed. Additionally, the Nbss and γNb5Si3 phases showcase the orientation
Xiao‐Wei Wang +6 more
wiley +1 more source
ABSTRACT Internal oxidation has been identified as an effective method for enhancing the strength of AgMg alloys. However, the concurrent occurrence of embrittlement remains inadequately understood, thus limiting their broader application. This study investigates the oxidation behavior of AgMg alloys with Mg concentrations ranging from 1 at% to 7 at ...
Hai‐Cheng Zhu +12 more
wiley +1 more source
用微量炸药接触爆炸的方法,研究了钨合金93W-4Ni-3Fe在高加载率条件下的断裂特性,通过宏、微观观察,以及与静态断裂特性相比较,发现随着加载率的增加,钨-钨界面裂纹增加 ...
周益春 +3 more
core +4 more sources
在断裂力学基础上建立起来的材料抵抗裂纹扩展断裂的韧性性能称为断裂韧性。断裂韧 性与其它韧性性能一样,综合反映了材料的强度和塑性,在防止低应力脆断选用材料时,
中国科学院老科技工作者协会工程力学分会
core +2 more sources
笔者分析了一起500 kV复合绝缘子脆断事故以及老化机理。该复合绝缘子脆断事故的特征与常见的脆断故障不同,在硅橡胶护套表面出现了部分贯通蚀孔,解剖后可以发现部分区域脱粘且在护套与芯棒交界面有漏电蚀痕。观察到故障复合绝缘子的宏观与微观交界面均存在一定的质量问题。使用傅氏变换红外光谱分析芯棒材料,证明在芯棒材料中存在玻璃化侵蚀,离子交换以及水解等老化过程。最后结合试验结果,分析了此类由于水份侵入而造成的老化现象,并建议在线监测中需关注复合绝缘子交界面质量。
冉学彬 +5 more
doaj
针对氧化锌非线性电阻片制造过程中隐性开裂的问题,采用金相显微镜等方法,对开裂断面的显微结构形貌、受力方式进行分析验证,探究了塑性开裂和脆性开裂两种隐性开裂的机理以及隐性开裂发生的时段。结果表明,氧化锌非线性电阻片发生隐性开裂的主要形式是在排结合剂之后发生的脆性开裂,这种开裂方式是在受力磕碰后,早期表现为非常隐蔽的微裂纹,后经高温烧结裂纹进一步扩展,最后受磨片剪切应力后开裂显现的一种失效模式。
张文刚 +5 more
doaj
Screening of β-thalassemia trait among pregnant women with NESTROFT
The morbidity of β-thalassemia major has forced medical professionals to formulate screening tests to effectively screen β-thalassemia trait (BTT) of which naked eye single tube osmotic fragility test (NESTROFT) is the most cost effective test.
Hitesh Sarda +2 more