Results 81 to 90 of about 827,566 (176)
Corrosion behavior of austenitic stainless steel in refinery wastewater ozone treatment system
Ozone catalytic oxidation technology is widely applied in the field of wastewater treatment of refining and chemical industries. However, there are some corrosion problems in the ozone treatment system during the long period operation, especially in ...
YANG Yanjia +6 more
doaj +1 more source
Even expensive 10K and 14K gold earrings released measurable gold in cysteine‐modified artificial sweat, despite no detectable nickel. Surface gold content did not predict release, challenging assumptions that higher gold content means lower exposure. ABSTRACT Background Gold contact allergy is common, but its clinical relevance is often uncertain.
Mikkel Bak Jensen +5 more
wiley +1 more source
Beyond Bactericidal: Plasma Surface Engineering to Defeat Food Matrix‐Conditioning Layers
ABSTRACT The persistence of foodborne pathogens on industrial food contact surfaces continues to challenge global food safety despite advances in sanitation technologies. A central limitation of current antimicrobial strategies lies in their validation under simplified laboratory conditions that overlook the physicochemically driven formation of food ...
Rafael Bianchini Fulindi +2 more
wiley +1 more source
Manufacture by Selective Laser Melting & Physical Behaviour of Commercial 316L Stainless Steel [PDF]
Selective Laser Melting is one of the technologies used to fabricate 3D sample directly through high energy focused laser. This method has a high potential in fabricating biocompatible material 316L stainless steel for biomedical implant devices.
Nurul Kamariah, Md Saiful Islam +6 more
core +3 more sources
A corrosion device was established to simulate the service environment of stainless steel heat exchanger tubes in a gas water heater. The pitting corrosion behaviors on the inner walls of 444, 445 and 316L stainless steel tubes were investigated in a tap
Shen Chen +4 more
doaj +1 more source
Analysis of Oxide Inclusions on Medical Grade 316L Stainless Steel using Local Raw
The type of stainless steel that is most commonly used in bone implants is austenitic 316L stainless steel, which has an excellent corrosion resistance and high strength. The Center for Materials Technology, BPPT, in cooperation with a local industry,
I Nyoman Jujur +3 more
doaj +1 more source
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees +6 more
wiley +1 more source
Influence of Surface Structure on Corrosion Behaviour of Welded Stainless Steel AISI 316l
The work deals with influence of surface structure on corrosion behaviour of austenitic stainless steel AISI 316L welded by TIG method without filler. Surfaces of the welded stainless steel were modified by mechanical treatment methods (grinding, garnet ...
Tatiana Liptakova +3 more
core +1 more source
Sliding wear of a-C:H coatings against alumina in corrosive media [PDF]
This paper reports the results obtained from the study of friction and sliding wear in two corrosive solutions of an a-C:H coating deposited on 316L stainless against an alumina ball, employed as static counter part. Calculations of the values of the von
La Barbera Sosa, J.G. +16 more
core +1 more source
Ultrasonic Vibration Assisted Laser Processing: A Hybrid Paradigm for Extreme Surface Enhancement
ABSTRACT Traditional laser processing techniques offer many advantages, but they often encounter limitations such as heat‐affected zones, recast layers, residual tensile stresses, and poor surface finish. The integration of ultrasonic vibration (UV) presents a promising hybrid approach to overcome these challenges by introducing beneficial effects like
Aziz Ul Hassan Mohsan +6 more