Results 221 to 230 of about 6,394,824 (315)

Evidence for multi-Li<sup>+</sup> clustering in lithium-ion battery electrolytes. [PDF]

open access: yesNature
Stevenson JM   +18 more
europepmc   +1 more source

Sacrificial‐Layer‐Assisted Heat‐Affected‐Zone Suppression in Laser Patterning of PET for High‐Performance Flexible Devices

open access: yesAdvanced Functional Materials, EarlyView.
A removable sacrificial polymer layer engineers the thermal boundary condition during nanosecond laser ablation of PET, suppressing heat‐affected‐zone formation without relying on costly ultrafast lasers. This strategy enables deep, high‐aspect‐ratio trenches with no detectable heat‐affected zone, templating silver‐filled mesh electrodes with record ...
Mehdi Zarei   +3 more
wiley   +1 more source

Surface-driven size scaling of the lattice parameter, Debye-Waller coefficient and microstrain in nanocrystals. [PDF]

open access: yesActa Crystallogr A Found Adv
Subbareddy S   +5 more
europepmc   +1 more source

Nitride MXenes Beyond Carbides: Bridging the Gap Between Computational Prediction and Experimental Realization

open access: yesAdvanced Functional Materials, EarlyView.
Nitride MXenes remain constrained by a persistent gap between computational prediction and experimental realization. This Review identifies the thermodynamic, kinetic, and chemical barriers limiting their synthesis, critically evaluates emerging fabrication routes, and proposes a multidimensional computational‐experimental framework to accelerate the ...
Naresh Varnakavi, Masoud Soroush
wiley   +1 more source

Electrochemical Wiring of a Metal Nanofilament to Form a Molecular Junction. [PDF]

open access: yesJ Phys Chem Lett
Nishimuro S   +6 more
europepmc   +1 more source

Biodegradable 3D‐Printable and Coatable Antifouling Composites for Marine Applications

open access: yesAdvanced Functional Materials, EarlyView.
Marine biofouling damages submerged surfaces and raises greenhouse gas emissions. Biodegradable antifouling biocomposites were developed by hot‐mixing beeswax, Tween 80, and calcium stearate or stearic acid. Adjusting the component ratio enables processing via hot‐pressing, 3D‐printing, or dip‐coating.
Gabriele Corigliano   +17 more
wiley   +1 more source

Unique Role of Microstructure of a Bioimplant Zinc Alloy and Protein Content of Simulated Body Fluid in Corrosion and Fracture

open access: yesAdvanced Functional Materials, EarlyView.
BSA addition to physiological solutions enhances resistance of a Zn alloy to stress corrosion cracking (SCC) but reduces its corrosion resistance. Extended surface characterization explains the contrasting influences on corrosion and SCC. Unexpectedly, the alloy suffers transgranular SCC (TGSCC), despite extensive grain boundary precipitation. Thorough
RK Singh Raman   +9 more
wiley   +1 more source

Twistionics in halide perovskites. [PDF]

open access: yesNat Commun
Yin S   +14 more
europepmc   +1 more source

Defect‐Free Transfer Principles for Scalable, Thin Garnet‐Based Hybrid Solid Electrolytes in Solid‐State Batteries

open access: yesAdvanced Functional Materials, EarlyView.
Defect‐free transfer principles enable scalable fabrication of 15 µm‐thin garnet‐based hybrid solid electrolytes. Hansen solubility parameters correlate interfacial compatibility with coating, transfer, and impregnation behavior, guiding rational selection of slurry/substrate, binder/substrate, and binder/polymer electrolyte combinations.
Seul Gi Chu   +8 more