Results 41 to 50 of about 877,528 (163)
Thermomechanical Processing, Microstructure, and Mechanical Properties of Medium‐Mn Steel
The microstructure evolution and mechanical properties of a medium‐Mn steel are investigated after thermomechanical processing and isothermal holding at various temperatures. A fine multiphase structure of bainite, fresh or tempered martensite, and retained austenite are obtained.
Burak Barutçuoğlu +3 more
wiley +1 more source
Very High Cycle Fatigue Performance of Ductile Cast Iron With Different Microstructures
ABSTRACT The very high cycle fatigue performance of four ductile cast irons, a solid solution strengthened ferritic, ferritic‐pearlitic, and two austempered ductile cast irons, was investigated by ultrasonic fatigue testing under fully reversed loading conditions. The step‐stress fatigue testing method incorporating re‐use of runouts was employed, with
Max Ahlqvist +3 more
wiley +1 more source
Effect of Austempering and Martempering on the Properties of AISI 52100 Steel
The mechanical properties of steel decide its applicability for a particular condition. Heat treatment processes are commonly used to enhance the required properties of steel. The present work aims at experimentally investigating the effect of austempering and martempering on AISI 52100 steel. Different tests like microstructure analysis, hardness test,
P. Vamsi Krishna +5 more
wiley +1 more source
Properties investigation of austempered ductile iron
This work concerns microstructural and mechanical properties of an austempered ductile cast iron (ADI). The ductile iron material was produced by the sand mould casting technique.
Detwal, Sudhanshu, R, Deivanathan
core +1 more source
The first stage of this study investigates the precipitation of free ferrite from the austenite on fully austenitized ductile iron. Several sets of samples of low alloy ductile iron are fully austenitized and then cooled down to different temperatures ...
A. D. Basso +4 more
doaj +1 more source
A low‐carbon (0.23 wt%) carbide‐free bainitic steel is successfully developed with a total alloying addition of 4.9 wt%, which is relatively lower than alloying additions reported in similar category of steels. The present findings indicate that the currently designed low‐alloy steel composition is amenable to generation of nearly carbide‐free bainitic
Poulami Chakraborty +8 more
wiley +1 more source
Taking into account the importance of the amount of bainite phase on the microstructure of cast irons and its influence on the improvement of mechanical properties, this research selected an alloy of gray cast iron containing Nickel‐Molybdenum and conducted the austenitising and austempering processes at 900°C and 400°C for 60 minutes, respectively ...
A. R. Kiani-Rashid +4 more
wiley +1 more source
Characteristics of ADI Ductile Cast Iron with Single Addition of 1.56% Ni
The results of examinations of microstructure and an analysis of its impact on selected mechanical properties of austempered ductile iron (ADI) were presented in the paper.
Mrzygłód B. +4 more
doaj +1 more source
Modeling of austempered ductile iron using discrete signals [PDF]
Austempered ductile iron is a perfect constructional material. Its unique properties combining high strength with good elongation follow from the material’s structure, in which a special role is played by a metallic matrix.
Andrzej Kochański +3 more
doaj +1 more source
The Effect of Cryogenic Treatment on W360 and E38K Hot Work Tool Steels
The cryogenic treatment facilitates the transformation of retained austenite to martensite to an undetectable limit, with about 3 times higher amount of the carbide precipitation for both steel types. Both steel types exhibit almost similar impact energy values at room temperature, but E38K steel has 2 times higher energy at 350 °C.
Caner Kiraz, Burak Birol, Ahmet Sağın
wiley +1 more source