Results 71 to 80 of about 5,040 (244)

The Effect of Cryogenic Treatment on W360 and E38K Hot Work Tool Steels

open access: yessteel research international, Volume 95, Issue 9, September 2024.
The cryogenic treatment facilitates the transformation of retained austenite to martensite to an undetectable limit, with about 3 times higher amount of the carbide precipitation for both steel types. Both steel types exhibit almost similar impact energy values at room temperature, but E38K steel has 2 times higher energy at 350 °C.
Caner Kiraz, Burak Birol, Ahmet Sağın
wiley   +1 more source

Microstructural Characterization and Some Mechanical Behaviour of Low Manganese Austempered Ferritic Ductile Iron [PDF]

open access: yes, 2017
This work studied the microstructural characterization and mechanical behavior of low manganese Austempered Ductile Iron (ADI), with a view to improve the properties of iron and to increase the areas of applications.
Abioye, Abiodun A.   +4 more
core   +2 more sources

Determining Factors of Grain Size in Bainite Structure of Fe–2Mn–C Alloys

open access: yessteel research international, Volume 95, Issue 8, August 2024.
The crystallographic variants and effective grain sizes of bainitic ferrite in Fe–2Mn–C alloys with various carbon contents are determined by local orientation measurements. Decrease in transformation temperature is beneficial for grain refinement of bainite structure although effects of carbon content are different between low‐carbon and high‐carbon ...
Tadashi Furuhara   +2 more
wiley   +1 more source

Analisa Peningkatan Sifat Mekanik Material Ring Piston Top Kompresi Yamaha Jupiter Z Dengan Proses Heat Treatment [PDF]

open access: yes, 2013
Terdapat dua produk suku cadang ring piston di pasaran, yaitu ring piston produk keluaran pabrikan resmi (genuine parts) dan ring piston barang kualitas menyerupai barang pabrik resmi disebut kualitas 1 disingkat KW 1.
Krisdianto, H. E. (Herawan)   +2 more
core  

The Austempering Kinetics, Microstructural Development and Processing Window in the Austempered, FE-3.2C-4.8AL Compacted Graphite Cast Iron

open access: yesIranian Journal of Materials Science and Engineering, 2020
In the present study, austempering heat treatment was performed on compacted graphite aluminum cast iron with the chemical composition of 4.8%wt Al, 3.2%wt C, 0.81%wt Ni, 0.37%wt Mn, and 0.02%wt Mg.
A. Kazazi   +2 more
doaj  

Investigation of Transient Nucleate Boiling Processes and Their Practical Use in Heat Treating Industry [PDF]

open access: yes, 2017
In the paper transient nucleate boiling process is widely discussed. It's unknown previously and investigated by author characteristics create a basis for designing of new technologies which allow receiving super strengthened materials.
Kobasko, N. (Nikolai)
core   +2 more sources

Microstructural evolution during austempering of a ASTM A-532 CLASS III type high chromium white cast iron undergoing abrasive wear

open access: yesRevista Facultad de Ingeniería, 2017
This paper studies the influence of variables such as holding temperatures and times during austempering of High Chromium White Cast Iron (HCWCI), with the following chemical composition: Cr 25 %, C 3 %, Si 0.47 %, Mn 0.74 % and Mo 1.02 %. The aim of the
Oscar Fabián Higuera-Cobos   +4 more
doaj   +1 more source

Microstructure and mechanical behaviors of grinding balls produced by dual matrix structure two-step austempering process

open access: yesJournal of Materials Research and Technology, 2020
The austempered ductile iron (ADI) grinding balls were austenitized at 900 °C for 2 h and then incomplete quenched in a sodium silicate solution for 100 s, after that austempered in an isothermal furnace at 230 °C for 1 h.
Hongyu Zhou, phD   +8 more
doaj   +1 more source

Effect of copper on the properties of austempered ductile iron castings [PDF]

open access: yes, 2012
Two types of ductile iron has been taken for the present investigation. Both austempering time and temperature are considered as the main variables for structure property correlation of Austempered Ductile Iron. The two types of spheroidal graphite iron (
Behera, Gourahari, Sohala, Soumya Ranjan
core  

Home - About - Disclaimer - Privacy