Results 141 to 150 of about 24,193 (277)
The effect of process of warm-forging at 880 ~ 930 °C on growth of austenite grain of gear steel 20CrMnTiH3 is analyzed by examination of physicochemistry and original material austenite grain size to get that the austenite of steel is easy abnormally ...
白瑞娟 +5 more
doaj
Austenite grain refinement enhances strength and toughness by producing refined hierarchical structure with dense high-angle grain boundaries. Yet, the contributions of distinct types of boundaries remain unclear.
Zhan Gao +7 more
doaj +1 more source
Laser welding of duplex stainless steel disrupts phase balance, promotes nitride precipitation, and reduces fatigue resistance. Postweld heat treatment restores austenite and dissolves nitrides, but the resulting crystallography and phase morphology still impair fatigue performance.
Aparecida Silva Magalhães +6 more
wiley +1 more source
Prebending of 304L/Q345R cladded plates significantly alters the subsequent weld thermal cycle and modifies the local interfacial microstructure. Combined electron backscatter diffraction (EBSD) and microscopy analysis demonstrates that deformation twinning, martensitic transformation, and defect initiation are concentrated at the trimaterial junction,
Ali Fahem +2 more
wiley +1 more source
Dependency of phase transformation on the prior austenite grain size and its influence on welding residual stress of S700 steel [PDF]
Abdel Wahab, Magd +3 more
core +1 more source
A double intercritical annealing strategy is proposed to tailor the multiphase microstructure and mechanical response of a medium‐Mn steel. The treatment produces an ultrafine mixture of ferrite, martensite and multiple austenite populations with graded thermal and mechanical stability, formed through austenite reversion and controlled retransformation.
Mattia Franceschi +3 more
wiley +1 more source
This work uses high‐temperature dilatometry to examine how the tramp elements Cu, Ni, and Sn affect the deformability of non‐metallic inclusions and matrix in quench‐and‐temper steel. Mg‐bearing inclusions deform less than Mg‐free ones. Copper lowers formability. Nickel increases deformability.
Julian Cejka +3 more
wiley +1 more source
Paint baking of resistance spot welded joints of 2.0 GPa warm‐stamped medium‐Mn steel activates low‐temperature tempering, forming fine cementite in the fusion zone and enhancing toughness. Crack propagation resistance increases, shifting the failure mode from partial interfacial to complete pullout, with peak load and energy absorption rising ...
Sunusi Marwana Manladan +8 more
wiley +1 more source
An accurate moving boundary model for volume diffusion containing boundary conditions from trans‐interface diffusion (TID) simulates the austenite growth during cooling. TID of Cr, Mo, N and Ni enhance growth kinetics. Without TID, compositions of the interface region change, decreasing the driving force for growth and finally causing numerical ...
A. Salwén +3 more
wiley +1 more source
This review explains how impurities from recycled scrap affect steel production and performance. Even small amounts (far below 1%) of these impurities can change how steel behaves during fabrication but also affect the properties of the end product. With better understanding and targeted countermeasures, these challenges can be managed, enabling wider ...
Oleksandr Glushko, Ronald Schnitzer