Results 101 to 110 of about 25,456 (225)

Microstructure and Shear Strength of Brazing TiAl/Si3N4 Joints with Ag-Cu Binary Alloy as Filler Metal

open access: yesMetals, 2018
Vacuum brazing of TiAl intermetallic alloy to Si3N4 ceramics was performed using Ag-28Cu (wt.%) filler alloy. The brazing joints obtained at different brazing temperatures were studied in this work. The microstructure and the shear strength were analyzed
Duo Dong   +5 more
doaj   +1 more source

Split glass tube assures quality in electron beam brazing [PDF]

open access: yes, 1966
Sealed enclosure of heat-resistant glass tubing and silicone rubber molds provide good visibility for electron beam brazing of metal tubes in an inert gas atmosphere. The glass tubing and rubber molds, which are bonded together, are easily applied to and
Kressin, W. J.
core   +1 more source

Microstructure and brazing properties of Ag20Cu35Zn(43.5-x-y)MnxSnyNi1.5 foil-filler brazing alloy

open access: yesHanjie xuebao
The influence of the addition of Mn and Sn elements on the microstructure, melting characteristics, and wettability of low-silver Ag20Cu35Zn(43.5-x-y)MnxSnyNi1.5 brazing alloys was investigated, and the content of Mn and Sn elements in the brazing alloys
Xuecheng WANG   +4 more
doaj   +1 more source

Metallurgical interactions in solid/liquid diffusion couples of AA4343/AA3xxx/AA4343 layered aluminum sheet

open access: yesJournal of Materials Research and Technology
The effect of pre-stretching on solid-liquid interaction, microstructure and brazing performance of AA4343/AA3xxx/AA4343 layered aluminum sheet during brazing at the atomic level (solid solution), nanoscale (dislocation) and micron level (grain boundary)
Zhipeng Yuan   +11 more
doaj   +1 more source

Method of making a rocket nozzle [PDF]

open access: yes, 1969
A method is described for forming the interior of a nozzle having uneven walls so that a throat of smooth converging and diverging sides is provided for passing flow.
Campbell, D. H.
core   +1 more source

Brazing

open access: yesBrazing
identifier:oai:t2r2.star.titech.ac.jp ...
openaire   +2 more sources

Tungsten wire and tubing joined by nickel brazing [PDF]

open access: yes, 1965
Thin tungsten wire and tungsten tubing are brazed together using a contacting coil of nickel wire heated to its melting point in an inert-gas atmosphere.

core   +1 more source

An Investigation on Corrosion Behavior of a Multi-layer Modified Aluminum Brazing Sheet

open access: yesMATEC Web of Conferences, 2016
The corrosion behavior of a multi-layer modified aluminum brazing sheet (AA4045/3003Mod./AA7072/AA4045) was investigated. The results shows that, the existence of BDP, which forms at the interface between clad and core layer during brazing, changes the ...
Liu Wei   +3 more
doaj   +1 more source

Work on PETS Developed at CIEMAT

open access: yes, 2012
CIEMAT has been working on the RF power extractor so-called PETS (Power Extraction and Transfer Structure) for the CLIC Test Facility 3 (CTF3) since 2007. The first contribution has been installed at the Test Beam Line (TBL).
Aragon, Fernando   +11 more
core  

Tube-to-header joint for bimetallic construction [PDF]

open access: yes, 1967
Design advantages of bimetallic construction enables an all-welded bimetallic joint to be made from the accessible header side of the tube-to-header joint.
Lessmann, G. G., Stoner, D. R.
core   +1 more source