Results 121 to 130 of about 49,671 (256)
High‐Performance Bio‐Glue From the Berries of a Parasitic Plant
We report a fully bio‐based adhesive derived primarily from a (poly)saccharide extract obtained from the berries of the hemi‐parasitic plant mistletoe (Viscum album), supplemented with tannic and malic acid without any further chemical functionalization.
Ufuk Gürer +8 more
wiley +1 more source
Intrinsically Stretchable Piezoelectric Nanocomposites for Artificial Ultrasonic Sensory Synapse
Applying ultrasonic stimulations to a soft‐stretchable underwater piezoelectric sensor based on the soft‐stretchable nanocomposite from the thermal cross‐linking between the ─C─F group of P(VDF‐TrFE) and the ─NH2 group of (PEG‐diamine) with incorporating amine‐terminated BTO@APTES nanofillers on the soft PDMS substrates generated high piezoelectric ...
Trung Dieu Do +11 more
wiley +1 more source
Flax Composites With Improved Interfacial Strength Through Microbially Induced Mineral Precipitation
A bio‐inspired biomineralization strategy introduces an additional hierarchy to flax fiber composites. By controlling microbe‐mediated mineral particle deposition through tuned salt concentrations, stress transfer within the natural fiber composite is enhanced.
Deniz Sayinbas +5 more
wiley +1 more source
Ceramic‐based V2O5/Fe3O4 hybrid films are shaped into butterfly‐proboscis‐inspired microscroll actuators. Magnetic triggering initiates unrolling, while geometry‐programmed elastic strain energy drives rapid recoil, enabling fast, reversible, durable, and load‐bearing actuation under near‐field magnetic stimulation.
Semi Kim +5 more
wiley +1 more source
Brittle or Quasi-Brittle Fracture of Engineering Materials: Recent Developments and New Challenges
F. Berto +4 more
doaj +1 more source
Interfacial Failure and Self‐Healing in Solid‐State Batteries
Dynamic interfacial self‐healing offers an adaptive route to mitigate coupled mechanical, chemical, and electrochemical degradation in solid‐state batteries. This review connects evolving interfacial failure mechanisms with physical‐flow, chemical‐restoration, stimuli‐responsive, and electric‐field‐assisted repair strategies, highlighting targeted self‐
Xinxin Zhu +8 more
wiley +1 more source
The mechanical performance of nanocellular polyetherimide cannot be explained by nanoporosity alone. It is shown that CO2 saturation and desorption leave a distinct mechanical signature in the glassy matrix before foaming. This matrix contribution provides a new route to understand and optimize the brittle to ductile transition in nanocellular polymers.
Félix Lizalde‐Arroyo +7 more
wiley +1 more source
Calculation method for brittle fracture of functional gradient materials
Combined the phase field model with the wavelet dummy node-virtual crack closure technique (WDN-VCCT) used for stress intensity factors (SIFs) calculation.
Cong Qi, Ai-guo Pi
doaj +1 more source
A thermoreversible gelatin‐based gel forms a soft, conformal bioelectronic interface on complex biological surfaces. The flowable precursor penetrates hair‐dense regions, solidifies in situ, and maintains low impedance through adaptive contact and hydration retention.
Ruinan Hao +9 more
wiley +1 more source