Results 11 to 20 of about 539,943 (266)
This study investigated the effect of stress on the microstructure evolution of austenitic stainless steels (316L SS and 304 SS) subjected to cavitation erosion and cavitation erosion-corrosion.
Ye Tian +7 more
doaj +4 more sources
Cavitation erosion by shockwave self-focusing of a single bubble. [PDF]
Highlights • An intensified collapse by self-focusing of shockwaves emitted during the collapse is proposed as main mechanism of cavitation erosion of hard materials.• Cavitation erosion occurs only for bubble collapses at close stand-off below γ≲0.2 ...
Reuter F, Deiter C, Ohl CD.
europepmc +4 more sources
The impact of cavitation erosion behavior on different metals in a water flowing system was investigated experimentally. A flowing system of water was built and a transparent observation window is designed to capture the cavitation flow.
Jie He +4 more
doaj +2 more sources
Degradation and Protection of Materials from Cavitation Erosion: A Review. [PDF]
The phenomena of cavitation and cavitation erosion affect hydraulic machines, increasing their maintenance costs. Both these phenomena and also the methods of preventing the destruction of materials are presented.
Krella AK.
europepmc +2 more sources
The influence of sulphide on the ultrasonic cavitation erosion-corrosion behaviors of HVOF-sprayed WC-Cr3C2-Ni coating. [PDF]
Highlights • Effect of sulphide on ultrasonic cavitation erosion-corrosion (UCE-C) of WC-Cr3C2-Ni coating was studied.• Under high sulphide concentration, the coating had certain resistance to UCE-C in the early stage of cavitation erosion.• In the ...
Shi X, Cui D, Wei Z, Hong S.
europepmc +2 more sources
A Review of Cavitation Erosion on Pumps and Valves in Nuclear Power Plants. [PDF]
The cavitation erosion failure of pumps or valves induces the low efficiency and reduced service life of nuclear reactors. This paper reviews works regarding the cavitation erosion of pumps and valves in the nuclear power industry and academic research ...
Gao G, Guo S, Li D.
europepmc +2 more sources
Effect of Initial Surface Scratches on the Cavitation Erosion Behavior of 316L Stainless Steel Substrates and 316L Stainless Steel Coatings. [PDF]
Rough surfaces have been widely considered as negative factors affecting cavitation erosion resistance. However, this study presented the opposite result.
Lu P +7 more
europepmc +2 more sources
Herein, cavitation erosion tests were carried out on 2205 and 2507 duplex stainless steels (DSSs) in distilled water and artificial seawater using ultrasonic cavitation erosion equipment.
Yapeng Wu, Ying Lian, Yang Li, Mao Feng
doaj +1 more source
An understanding of the cavitation erosion behavior and mechanisms of high‑nitrogen austenitic stainless steel is of interest for scientific and economic reasons.
Zhenhua Wang, Bing Zhang
doaj +1 more source
Cavitation Erosion Risk Assessment for a Marine Propeller Behind a Ro-Ro Container Vessel
A novel cavitation erosion risk model, developed by Schenke et al. ["On the relevance of kinematics for cavitation implosion loads," Phys. Fluids 31, 052102 (2019)], is applied to compute the cavitation implosion loads.
T. Melissaris +2 more