Results 191 to 200 of about 15,676,159 (315)
This study examines how helicoidal architectures with different porosities respond to bending. Adjusting layer angle and spacing in 3D‐printed polymers reveals clear tradeoffs between stiffness, strength, and energy absorption. Experiments and simulations highlight designs that distribute stress effectively, offering pathways for optimizing lightweight
Praveenkumar Subhash Patil +2 more
wiley +1 more source
Mass density governs the protective behavior of oxide layers on nuclear fuel cladding. Ptychographic X‐ray computed tomography measures zirconium oxide grown on Zircaloy‐4 under reactor and autoclave conditions, revealing nearly identical bulk densities of 5.1 ± 0.80 g cm−3.
Okan Yetik +9 more
wiley +1 more source
Sustainable RC Beams with Agricultural Waste Fine Aggregate and Glass Powder: Structural Evaluation under Bending. [PDF]
Ali ZM +4 more
europepmc +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
Experiments and thermophysical simulations were conducted to investigate the electron beam powder bed fusion electron beam (PBF‐EB/M) process for the γ′‐strengthened nickel‐based superalloy Inconel 738LC. The results demonstrate the impact of process‐induced microstructural variations on high‐temperature mechanical behavior, providing a basis for ...
Jan Niklas Petenati +11 more
wiley +1 more source
Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi +5 more
wiley +1 more source
Thermodynamic Criterion for Quasi-Static Tearing of Elastic and Elastic-Plastic Fracture Specimens, and Its Validation from the Empirical Structure of Load-Displacement Diagrams. [PDF]
Snyder VA.
europepmc +1 more source
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley +1 more source
Plastic Shrinkage Cracking of Full-Scale Concrete Slabs Under Field-Production Conditions: Observations on Mix Design, Environmental Exposure and Curing. [PDF]
Rutkowska G +3 more
europepmc +1 more source