Results 171 to 180 of about 222,942 (303)
Nickel‐based alloys are widely used in high‐temperature applications due to their excellent mechanical strength and oxidation resistance. However, properties such as high‐temperature strength and pronounced work‐hardening make them difficult to machine.
Soheil Rooein +2 more
wiley +1 more source
The presented study focuses on the fracture behaviour of carbon‐bonded magnesia MgO–C refractories, where environmentally friendly fructose, collagen and lignin serve as temporary binding agents. The partial substitution of the source material with recycled MgO–C reduces the fracture resistance, which can be counteracted by the additional introduction ...
Marc Neumann +6 more
wiley +1 more source
Fatigue crack growth of glass fiber laminates polymer composites using vacuum bagging technique. [PDF]
Chaloob MK +3 more
europepmc +1 more source
Carbon‐free inert anodes are essential for decarbonizing aluminum electrolysis. This study investigates a recyclate‐based MgO‐316L steel composite anode tested under galvanostatic Hall–Héroult conditions in cryolite at 1000°C. Microstructural analysis reveals selective MgO fluorination, spinel and oxide layer formation, electrolyte infiltration, and ...
Serhii Yaroshevskyi +7 more
wiley +1 more source
Influence of connection configuration on the punching resistance of CFST column-RC slab systems under eccentric loading. [PDF]
Ghalla M +5 more
europepmc +1 more source
Powder Optimization Strategies for Binder Jetting Printing of BaTiO3 and Ba0,6Sr0,4TiO3 Ceramics
Powder optimization is investigated to enable binder jetting of BaTiO3 and Ba0.6Sr0.4TiO3 ferroelectric ceramics. The antagonistic relationship between flowability and binder compatibility is addressed through binder impregnation of granulated powders and fumed silica addition to fine powders.
Fanny Pruvost +4 more
wiley +1 more source
A Comprehensive Review on the Enhancement Mechanism of Fatigue Performance in Titanium Alloys via Laser Shock Peening. [PDF]
Zu Q, Yang J, Li J, Qi X, Yang X.
europepmc +1 more source
The formation of nonmetallic inclusions (NMIs) was investigated in this study, carrying out immersion tests for 30 min at a temperature of 1600°C with liquid high‐silicon electrical steel (Si ≈ 3 mass‐%) and different MgO–C refractories. Conventional MgO–C refractories were considered, as well as MgO–C refractories containing MgO–C recyclate and ...
Lukas Neubert +6 more
wiley +1 more source
Effect of dislocation slip on in-situ tensile fracture of vanadium alloys after helium/self-ion irradiation. [PDF]
Zhang Q +6 more
europepmc +1 more source
Assessing Altered Coating Adhesion on Plasma‐Deoxidized Surfaces Under Oxygen‐Free Conditions
This study demonstrates the effectiveness of atmospheric pressure plasma pretreatment in modifying silicon and stainless steel surfaces to improve adhesion. Argon‐hydrogen plasma increases surface roughness and improves adhesion strength, whereas pure argon results in smoother surfaces and structural changes.
Selina Raumel +6 more
wiley +1 more source