Results 91 to 100 of about 2,171,604 (298)
The crystal habit of pentaerythritol (PE) crystals is usually rod-shaped, which may lead to low bulk density and bad flowability compared with low aspect ratio crystals.
Wang Wei +11 more
doaj +1 more source
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
Binder‐free laser powder bed fusion of 8YSZ with a femtosecond laser is used to map process windows linking scan strategy, heat accumulation, and grain growth. Time‐resolved thermography and simulations reveal thermal regimes that enable continuous, vitrified, and fine‐grained 8YSZ surface layers without absorptive additives and demonstrate ...
Markus Kühn +5 more
wiley +1 more source
Crystal phase and morphology controlled synthesis of Fe2O3 nanomaterials
Crystal phase and morphology controlled synthesis of Fe2O3 ...
魏雪姣 +6 more
core
Surface morphology and deformation mechanism of single crystal copper treated by laser shock peening [PDF]
To study the relation between surface morphology and deformation mechanism of the target material under the shock, a flexible boundary loading, in laser shock peening(LSP), the macroscopic and microscopic surface morphology of a single crystal copper ...
王曦, 黄晨光, Liu YX, 吴先前
core +1 more source
This study examines Invar composites reinforced with titanium carbide (TiC) and titanium nitride (TiN) using laser powder bed fusion (LPBF). It presents the influence of reinforcements on microstructure, tensile properties, and thermal expansion. Results show that TiC effectively strengthens Invar while maintaining low thermal expansion, whereas TiN ...
Ayodeji Nathaniel Oyedeji +3 more
wiley +1 more source
Application of CO2 clathrate hydrate as a constituent of solid carbonated foods is an emerging new idea to utilize the large gas-storage capacity of this material.
Risa Tokunaga +4 more
doaj +1 more source
Rapidly Solidified High‐Strength Invar 36 Prepared by Planar‐Flow Melt Spinning
The Invar 36 alloy was rapidly solidified using the planar‐flow melt‐spinning technique. Ribbon samples with thicknesses ranging from 20 to 160 mm were produced. As the grain size of the ribbon decreased to sub‐micron levels, the hardness increased by more than 2 times.
Bekir Akgül, Mehmet Kul
wiley +1 more source
The crystal structure of 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazaiso-wurtzitane (CL-20) p-xylene solvate, and the solvent effects on the crystal faces of CL-20 were studied through a combined experimental and theoretical method.
Fanfan Shen +4 more
doaj +1 more source
Gallium microalloying redirects interfacial reactions in low‐temperature Bi–Sn solders from Cu–Sn toward Cu–Ga intermetallic formation. The resulting Cu–Ga layer suppresses intermetallic growth during thermal aging, alters fracture pathways, and improves interfacial stability.
Iva Králová +6 more
wiley +1 more source