Results 51 to 60 of about 1,768 (186)
Prebending of 304L/Q345R cladded plates significantly alters the subsequent weld thermal cycle and modifies the local interfacial microstructure. Combined electron backscatter diffraction (EBSD) and microscopy analysis demonstrates that deformation twinning, martensitic transformation, and defect initiation are concentrated at the trimaterial junction,
Ali Fahem +2 more
wiley +1 more source
Dissimilar metal welding is a popular process in very large coal and gold, power generation, and pulp and paper factories. It has mainly been applied to produce large boilers in sugar factories.
Jinkamon Luijan +2 more
doaj +1 more source
Paint baking of resistance spot welded joints of 2.0 GPa warm‐stamped medium‐Mn steel activates low‐temperature tempering, forming fine cementite in the fusion zone and enhancing toughness. Crack propagation resistance increases, shifting the failure mode from partial interfacial to complete pullout, with peak load and energy absorption rising ...
Sunusi Marwana Manladan +8 more
wiley +1 more source
The high‐strain‐rate behavior of resistance spot‐welded DP800–DP1000 joints is investigated. Results show that microstructural gradients across BM–HAZ–FZ govern hardness, strain rate sensitivity, and failure modes. While strength increases with strain rate, energy absorption is controlled by ductility, with DP800–DP800 joints showing superior ...
Pankaj Shrivastava, Velaphi Msomi
wiley +1 more source
Fatigue Strength Analysis of a Cladded Steel Subjected to Tensile Predeformation
ABSTRACT Cladded steels are a subset of layered metal composites in which a thin functional layer is bonded to a dissimilar substrate, thereby integrating the benefits of both constituent materials. However, the resulting heterogeneous properties of such layered metal composites collectively complicate deformation and fatigue behavior, making reliable ...
Marcel Krochmal +2 more
wiley +1 more source
ABSTRACT The fatigue and fracture behavior of self‐piercing rivet (SPR) joints between AA6016 aluminum sheets (1–2 mm) and DX54D steel (0.95 mm) was studied under 90°, 45°, and 0° multiaxial loading. Pure shear (90°) loading produced the highest fatigue strength, whereas multiaxial (45°) loading resulted in reduced performance, with pure tension (0 ...
Alan Woo +5 more
wiley +1 more source
It is known that some problems commonly arise when welding dissimilar metals, especially because it is more difficult to join dissimilar metals than similar metals.
Bensheng Huang +4 more
doaj +1 more source
It is shown that laser ablation pretreatment under oxygen‐free conditions enables copper–aluminium bonding at significantly lower deformation degrees and improved properties compared to mechanical brushing. Laser ablation further increases interface contact area and induces favourable residual stress states and microstructural compatibility ...
Khemais Barienti +11 more
wiley +1 more source
Joining of dissimilar materials by friction stir welding [PDF]
Welding is a process of joining materials into one piece. Welding is used extensively for pipe welding, aerospace, aviation, biomedical implants, fabrication of race cars, choppers, etc. Welding processes include thermal fusion joining processes and solid-state joining processes.
openaire +2 more sources
Friction stir welding (FSW) is a promising welding method to produce dissimilar joints between steel and aluminium. The formation of the intermetallic compound layer at the dissimilar joint interface affects the joint mechanical properties, which are ...
M Karthikeyan, Jonah