Results 201 to 210 of about 1,942,110 (351)

Mechanically Deposited Wear‐Resistant Amorphous Zr55Cu30Al10Ni5 Coatings

open access: yesAdvanced Engineering Materials, EarlyView.
Mechanically deposited from glassy ribbons, the Zr55Cu30Al10Ni5 amorphous coating formed a hard, continuous layer on AISI 1010 steel, tripling substrate hardness, lowering friction, and reducing wear. Despite its rough surface, it showed friction and wear behavior comparable to the crystalline alloy, highlighting its strong potential as a durable ...
Tales Ferreira   +8 more
wiley   +1 more source

Ear Keloids Treated with Postoperative Electrons: A Case Series

open access: yesSouth Asian Journal of Cancer
Pankaj Vats   +5 more
doaj   +1 more source

Electron Manipulation and Surface Reconstruction of Bimetallic Iron–Nickel Phosphide Nanotubes for Enhanced Alkaline Water Electrolysis

open access: gold
Xinqiang Wang   +14 more
openalex   +1 more source

Nitride‐Reinforced Metal Matrix Nanocomposite Powders Production by Plasma‐Assisted Thermochemical Treatment of Intermetallic Powders

open access: yesAdvanced Engineering Materials, EarlyView.
This study proposes a new methodology for producing metal matrix nanocomposites in the solid state. The process involves the plasma‐assisted thermochemical treatment of metallic alloy powders. As a proof‐of‐concept, TiN nanoparticles are synthesized directly on the surface of FeTi intermetallic powder particles, enabling the development of the ...
Deivison Daros Paim   +4 more
wiley   +1 more source

Off-Axis Electron Holography of In-Situ-Biased Highly-Doped p-AlGaAs/n-GaInP Junctions for Solar Cell Applications [PDF]

open access: yesBIO Web of Conferences
Mergner Vita   +7 more
doaj   +1 more source

Interaction between Molten Al‐Killed Mn–B Steel and Carbon‐Bonded MgO Refractories Based on Recyclates

open access: yesAdvanced Engineering Materials, EarlyView.
High‐temperature interactions between low‐sulfur Al‐killed Mn–B steel and MgO–C refractories (0 and 50 wt% recyclates) are studied via finger immersion tests (1600 °C). Surface‐active elements influence infiltration. MgO/CaS layer forms, along with spinel and calcium silicate.