Results 131 to 140 of about 43,335 (258)
Alloy Qualification for Producing Quench and Tempered Plate Steels with Extra‐Heavy Gage
This study develops alloy concepts for ultraheavy steel plates (>100 mm) with ≥690 MPa yield strength. Through dilatometry and Jominy testing, the effects of Mo, Ni, and B on hardenability are quantified. A synergy between 0.5% Mo and 0.5%–1.0% Ni ensures core strength at low cooling rates, while boron microalloying suppresses ferrite and promotes ...
Xabier Azpeitia +5 more
wiley +1 more source
An electrochemical method for determining hydrogen concentrations in metals and some applications [PDF]
An electrochemical method was developed for the determination of hydrogen in metals using the EG&G-PARC Model 350A Corrosion Measurement Console. The method was applied to hydrogen uptake, both during electrolysis and electroplating, and to studies of ...
Danford, M. D.
core +1 more source
This work demonstrates that replacing Ti with Nb in maraging steel forms nanoscale Nb–Mo particles along boundaries, strengthening the alloy without relying on Ti phases. Heat‐treatment tuning promotes uniform crystal orientation and balanced grain boundaries, enabling strong yet ductile behavior.
Mohamad Masoumi +14 more
wiley +1 more source
Environmental fatigue of an Al-Li-Cu alloy. Part 3: Modeling of crack tip hydrogen damage [PDF]
Environmental fatigue crack propagation rates and microscopic damage modes in Al-Li-Cu alloy 2090 (Parts 1 and 2) are described by a crack tip process zone model based on hydrogen embrittlement. Da/dN sub ENV equates to discontinuous crack advance over a
Gangloff, Richard P., Piascik, Robert S.
core +1 more source
Pre‐failure behavior of continuous post‐tensioned and post‐grouted beam in case of tendon failure
Abstract Grouted tendons are a common solution for long‐span bridge structures. The grout provides bond and corrosion protection for prestressing steel. However, if the grouting is defective, corrosion of the prestressing steel may initiate and eventually lead to tendon failure.
Olli Asp +2 more
wiley +1 more source
A novel bio‐based stabilizer system significantly improves the quality of polyolefin recyclates during multiple recycling cycles. ABSTRACT This study introduces a novel bio‐based stabilizer system for polyolefin recyclates that combines alditols with small amounts of α‐tocopherol as a sustainable alternative to conventional phosphite additives. The aim
Kim Hao Ng +3 more
wiley +1 more source
ABSTRACT Low‐voltage cables insulated with silicone rubber were harvested from three locations in the primary containment vessel of a boiling water nuclear power plant (NPP). Subsequently, the cable, which was placed in an ambient environment with a relatively higher temperature and the highest rate, was cut into four shorter ones.
Yoshimichi Ohki +2 more
wiley +1 more source
ABSTRACT Twelve metal artifacts from recent excavations at the Sasanian archaeological site of Jahāngir in western Iran have been analyzed. These items include both decorative and utilitarian artifacts. The samples were examined using micro‐X‐ray fluorescence (μ‐XRF), scanning electron microscopy with energy‐dispersive X‐ray spectroscopy (SEM‐EDS), and
Omid Oudbashi +2 more
wiley +1 more source
Effects of temperature and strain rate on the mechanical properties of T91 material tested in liquid lead bismuth eutectic [PDF]
ALMAZOUZI, A +2 more
core +1 more source
ABSTRACT The degradation of metallic materials due to hydrogen embrittlement (HE) poses critical challenges for structural reliability. Phase‐field models offer an energy‐based approach that does not require predefined crack paths and automatically determines crack initiation, growth, and coalescence.
Shaymaa Merheb +7 more
wiley +1 more source