Active Corrosion Protection of Sintered AA7075 Aluminum Alloy via Mn Powder Addition
AA7075 containing Mn‐rich particles is fabricated via spark plasma sintering using AA7075 and Mn powders. Corrosion resistance is evaluated through dip‐and‐dry tests using 0.1 M NaCl (pH 6.0), and mass loss decreases with increasing Mn addition. Mn‐rich particles function as a source of Mn ions, and formation of Mn‐accumulation films on Cu‐containing ...
Ko Ebina, Masashi Nishimoto, Izumi Muto
wiley +1 more source
Children-specific environmental protection strategies are needed in China. [PDF]
Zhang J +6 more
europepmc +1 more source
This review comprehensively evaluates extrusion‐based additive manufacturing for advanced ceramics, detailing feedstock options and key process parameters. By critically addressing defect mechanisms like porosity and cracking, the work highlights optimization strategies through machine learning and advanced postprocessing.
Meisam Bakhtiari +4 more
wiley +1 more source
The actual effect and mechanism of environmental protection taxes on carbon emission reduction: evidence from China. [PDF]
Luo J, Huang J, Zhang Y.
europepmc +1 more source
High‐Resolution Corrosion Fingerprinting of Alloy Libraries via Microdroplet Spectroelectrochemistry
Ionic‐liquid microdroplet spectroelectrochemistry enables stable, localized electrochemical measurements over extended timescales. By coupling impedance spectroscopy, wetting analysis, finite‐element simulations, and operando Raman spectroscopy, it disentangles geometrical and electrochemical effects, opening new opportunities for rapid corrosion ...
Ekaterina Kurchavova +3 more
wiley +1 more source
Correction: Environmental protection tax and green innovation of heavily polluting enterprises: A quasi-natural experiment based on the implementation of China's environmental protection tax law. [PDF]
Deng J, Yang J, Liu Z, Tan Q.
europepmc +1 more source
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
Linking carbon footprint methodologies and environmental protection via sustainable product development with a moderating role of regulatory compliance. [PDF]
Qalati SA +5 more
europepmc +1 more source
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees +6 more
wiley +1 more source
Enhancing Low‐Temperature Performance of Sodium‐Ion Batteries via Anion‐Solvent Interactions
DOL is introduced into electrolytes as a co‐solvent, increasing slat solubility, ion conductivity, and the de‐solvent process, and forming an anion‐rich solvent shell due to its high interaction with anion. With the above virtues, the batteries using this electrolyte exhibit excellent cycling stability at low temperatures. Abstract Sodium‐ion batteries
Cheng Zheng +7 more
wiley +1 more source