Results 111 to 120 of about 515,656 (287)
Environmental Scanning Electron Microscope: Some Critical Issues
In the environmental scanning electron microscope (ESEM), the gas flow around the main pressure limiting aperture establishes a density gradient through which the electron beam passes. Electron beam losses occur in this transition region and in the uniform gas layer above the specimen surface.
openaire +1 more source
Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han +5 more
wiley +1 more source
Enhanced Strength and Corrosion Resistance of Ti‐13Nb‐12Ta‐10Zr‐4Sn Alloy by Aging Treatment
This work systematically investigates the effect of aging treatment on mechanical properties and corrosion behavior of vacuum arc‐melted Ti‐13Nb‐12Ta‐10Zr‐4Sn alloy. Owing to the increased α″ martensite, strength and corrosion resistance were significantly enhanced by aging treatment.
Yuhua Li +5 more
wiley +1 more source
Viktoriia Shtefan, Thorgund Nemec, Ute Hempel, Annett Gebert and coworkers demonstrate that anodic treatment of Ti–Cu‐based metallic glass in a nontoxic pyrophosphate electrolyte forms a protective bilayered Ti/Zr‐oxide film enriched with Cu nanocrystals.
Viktoriia Shtefan +8 more
wiley +1 more source
The environmental scanning electron microscope (ESEM) - theory and applications
The environmental scanning electron microscope (ESEM) allows direct observation of specimens in their natural state, without the need for elaborate sample preparation techniques. Recent technical developments allow the detection of various signals generated by the specimen, such as secondary and backscattered electrons, cathodoluminescence, and x-rays.
openaire +1 more source
Graphene nanoplatelet (0.1 wt.%) reinforcement significantly enhances the performance of β Ti‐28Nb‐35.4Zr alloy. Grain refinement, reduced water contact angle, and improved surface characteristics promote osteoblast adhesion and complete surface coverage after 7 days.
Khurram Munir +5 more
wiley +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
Cathodic Cage Plasma Deposition of Nanostructured Cu–Fe–Se Coatings on Poly(methyl Methacrylate)
Nanostructured Cu–Fe–Se coatings are deposited on PMMA by a modified cathodic cage plasma process, enabling low‐temperature deposition on polymer substrates. A transition from discontinuous to compact morphology is observed with temperature, with optimal properties at 200°C, where improved CuFeSe2‐type bonding, lowest sheet resistance, and favorable ...
V. S. S. Sobrinho +8 more
wiley +1 more source
The Polonnaruwa meteorite: oxygen isotope, crystalline and biological composition
Results of X-Ray Diffraction (XRD) analysis, Triple Oxygen Isotope analysis and Scanning Electron Microscopic (SEM) studies are presented for stone fragments recovered from the North Central Province of Sri Lanka following a witnessed fireball event on ...
Gibson, Carl H. +9 more
core
Environmental Scanning Electron Microscopic Study Of Electron Impacted High Explosive Materials [PDF]
S K Hait +4 more
openaire +1 more source