Results 181 to 190 of about 19,386 (222)
Some of the next articles are maybe not open access.

Sulfomaleation of EPDM polymers

Macromolecules, 1987
Introduction de groupes polaires fonctionnels a l'aide d'anhydride thiomaleique et de ses ...
Warren A. Thaler   +2 more
openaire   +1 more source

Improved Aging Performance of Virgin EPDM Roof-Sheeting Compounds with Amine-Devulcanized EPDM Weatherstrip Material

Rubber Chemistry and Technology, 2008
Abstract Sulfur-cured EPDM building-profile material was reclaimed in a co-rotating twin-screw extruder using hexadecylamine as reclaiming aid. This reclaim was blended with increasing amounts of a virgin EPDM roof-sheeting masterbatch and cured at temperatures allowing for a reversion-free vulcanization.
Dijkhuis, K.A.J.   +3 more
openaire   +2 more sources

Thermoplastic Elastomer Based on PP/EPDM/ENR25 and PP/EPDM/NR Blends

Polymer-Plastics Technology and Engineering, 2004
Abstract A series of ternary blends of polypropylene (PP)/ethylene-propylene-diene terpolymer (EPDM)/natural rubber (NR) and PP/EPDM/epoxidized natural rubber (ENR25) were prepared in a laboratory internal mixer at 180°C and a rotor speed of 50 rpm. The mechanical properties, oil resistance, and morphological studies of PP/EPDM/NR and PP/EPDM/ENR25 ...
null Halimatuddahliana, H. Ismail
openaire   +1 more source

Spotlight on EPDM Elastomers

Polymer-Plastics Technology and Engineering, 1992
Abstract Etylene-propylene diene monomer (EPDM) rubbers have become widely recognized as an important class of elastomers in an enormous variety of consumer-type products. Typical examples where this material is used include seals around automotive doors, trunks, and windows; hosing materials used in automotive radiator applications, ply-roofing ...
openaire   +1 more source

AC Brealdown Studies on Crosslinked EPDM

IEEE Transactions on Electrical Insulation, 1976
The electromechanical breakdown mechanism1, 2 has long been presumed to be responsible for the low dielectric strength of elastomers when tested with parallel-plate-type elec­trodes. In this breakdown model, the compression force generated by the applied voltage, V, deforms the polymer slab from the original thickness d 0 to a thickness d.
openaire   +1 more source

Sinteza graft kopolimera EPDM-g-PS i priprava mješavine SAN/EPDM

2001
Graft polimerizacija stirena na etilen-propilen-dienski kopolimer (EPDM) provedena je u heptanu uz inicijator benzoil peroksid. Sadržaj homopolimera EPDM-a i PS-a u pripravi graft kopolimera EPDM-g-PS je 1:1. Reakcijska smjesa polimera razdvojena je na homopolimer i graft kopolimer i određena je konverzija te njihovi udjeli.
openaire   +1 more source

EPDM SEAL

1999
Peter A. Ciullo, Norman Hewitt
openaire   +1 more source

Use of Fine EPDM Powder in EPDM-based Rubber Mixes

International Polymer Science and Technology, 2010
M.V. Adov   +3 more
openaire   +1 more source