Results 151 to 160 of about 3,615 (234)
High‐temperature interactions between low‐sulfur Al‐killed Mn–B steel and MgO–C refractories (0 and 50 wt% recyclates) are studied via finger immersion tests (1600 °C). Surface‐active elements influence infiltration. MgO/CaS layer forms, along with spinel and calcium silicate.
Matheus Roberto Bellé +5 more
wiley +1 more source
The thermal diffusivity of MgO‐C refractories is highly sensitive to sample preparation and processing procedures. In this article, the effects of coking sequence, machining conditions, structural inhomogeneity, and graphite coating application on measurements using laser flash apparatus are systematically investigated.
Luyao Pan +4 more
wiley +1 more source
Spontaneous flexibility, attentional set shifting and cognitive control in men with alcohol dependence. [PDF]
Zawadzka E, Domańska Ł.
europepmc +1 more source
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
Adaptation of the Intelligence Structure Test, Latvian version: psychometric properties. [PDF]
Jokste I +4 more
europepmc +1 more source
This study investigates the tribological response of 60NiTi alloy under dry, water‐lubricated and high‐temperature conditions. The alloy exhibits decreasing wear volume and friction with increasing temperature due to the formation of protective oxide layers. The work clarifies dominant wear mechanisms and demonstrates the suitability of 60NiTi for high‐
Anthony Onyebuchi Okoani +2 more
wiley +1 more source
Automatic- and Transformer-Based Automatic Item Generation: A Critical Review. [PDF]
Sommer M, Arendasy M.
europepmc +1 more source
Stabilization of L‐PBF Ni50.7Ti49.3 under low‐cycle loading was investigated. Recoverable strain after cycling was dependent on the amount of applied load. Recovery ratio was 53.4% and 35.1% at intermediate and high load, respectively. The maximum total strain reached 10.3% at a high load of 1200 MPa.
Ondřej Červinek +5 more