Cooling-Regime Effects on the Residual Mechanical Properties, Hardness and Fracture Characteristics of Fire-Exposed Hardox Abrasion-Resistant Steels. [PDF]
Zeybek Ö +4 more
europepmc +1 more source
Fracture behavior and interfacial toughening mechanisms of SiC microfiller-reinforced gossypium/glass-epoxy hybrid composites for automotive structural applications. [PDF]
Arul M +5 more
europepmc +1 more source
Results of an experimental estimation of the crack closure stress, using electron fractography and laser interferometry for CT specimens of an aluminium-copper alloy are presented in this paper. Crack closure stress was estimated at stress ratios of 0.1,
Ashbaugh, NE +7 more
core
Experimental investigation of tensile properties and fracture behavior of ophthalmic sutures under straight, knotted, and looped configurations: Vicryl, nylon, and polypropylene. [PDF]
Dalai R +6 more
europepmc +1 more source
Fatigue Performance and Failure Loads of Composition-Gradient Multilayer Zirconia: Partial-Coverage Restorations Versus Single Crowns at Different Thicknesses. [PDF]
Spitznagel FA +7 more
europepmc +1 more source
Relationship Between Fracture Toughness and Fracture Mirror in Modern Polymer-Based Dental Composites. [PDF]
Ilie N.
europepmc +1 more source
From cracks to informed circularity: Mechanics-guided decisions via high-throughput in situ failure analysis of recycled plastics. [PDF]
Sun D, Xu Y, Athanasiou CE.
europepmc +1 more source
Characterization of PC-ABS and PETG Multi-Material Laminates Fabricated by MEX Method. [PDF]
Nainaragaram Ramasamy M +8 more
europepmc +1 more source
Mechanical Anisotropy and Fatigue Behavior of 3D-Printed Dentures: A Comparison with CAD/CAM Milled Bases After Thermomechanical Aging. [PDF]
Alkhodary MA +5 more
europepmc +1 more source