Results 101 to 110 of about 13,679 (229)
The effect of microstructure on the fracture toughness of titanium alloys [PDF]
The microstructure of the alpha titanium alloy Ti-5Al-2.5Sn and the metastable beta titanium alloy Beta 3 was examined. The material was from normal and extra low interstitial grade plates which were either air-cooled or furnace-cooled from an annealing ...
Low, J. R., Jr. +2 more
core +1 more source
Tensile and fatigue properties of Inconel 718 at cryogenic temperatures [PDF]
Tests to determine the tensile and fatigue properties of Inconel 718 at cryogenic temperatures show that the alloy increases in strength at low temperatures, with very little change in toughness. The effect of surface finish and grain size on the fatigue
Malin, C. O., Schmidt, E. H.
core +1 more source
Damage mechanisms in bithermal and thermomechanical fatigue of Haynes 188 [PDF]
Post failure fractographic and metallographic studies were conducted on Haynes 188 specimens fatigued under bithermal and thermomechanical loading conditions between 316 and 760 C.
Halford, Gary R., Kalluri, Sreeramesh
core +1 more source
A study of hydrogen environment effects on microstructure property behavior of NASA-23 alloy and related alloy systems [PDF]
This work is part of the overall advanced main combustion chamber (AMCC) casting characterization program of the Materials and Processes Laboratory of the Marshall Space Flight Center.
Diwan, Ravinder M.
core +1 more source
A fundamental approach to adhesion: Synthesis, surface analysis, thermodynamics and mechanics [PDF]
The effects of composites as adherends was studied. Several other variables were studied by fractography: aluminum powder adhesive filler, fiber glass cloth scrim or adhesive carrier, new adhesives PPQ-413 and LARC-13, and strength-test temperature. When
Dwight, D. W., Wightman, J. P.
core +2 more sources
Fractography, elastic modulus and oxidation resistance of novel metal-intermetallic Ni/Ni 3Al multilayer films [PDF]
Novel metal–intermetallic Ni/Ni3Al multilayer films are synthesized by a magnetron sputtering technique. The fractography, elastic modulus, and the oxidation resistance of the multilayer films are studied by a series of experimental tests.
Mathur, S +4 more
core
Spiral cracks in drying precipitates
We investigate the formation of spiral crack patterns during the desiccation of thin layers of precipitates in contact with a substrate. This symmetry-breaking fracturing mode is found to arise naturally not from torsion forces, but from a propagating ...
A. E. Tucker +20 more
core +1 more source
Testing methods and techniques - A compilation [PDF]
Nondestructive test methods and techniques including computer programs and data ...
core +1 more source
Register of experts for information on mechanics of structural failure [PDF]
This register is comprised of a list of approximately 300 experts from approximately 90 organizations who have published results of theoretical and/or experimental research related to six problem areas in the mechanics of structural failure: (1) life ...
Carpenter, J. L., Jr., Stuhrke, W. F.
core +1 more source
High-boron 9–10% chromium martensitic steels are an advanced material for manufacturing various com-ponents of thermal power units in coal-fired power plants operating under ultra-supercritical steam conditions (up to ...
Ivan S. Brazhnikov +1 more
doaj +1 more source