Results 111 to 120 of about 13,679 (229)

Scaling of Crack Surfaces and Implications on Fracture Mechanics

open access: yes, 2000
The scaling laws describing the roughness development of crack surfaces are incorporated into the Griffith criterion. We show that, in the case of a Family-Vicsek scaling, the energy balance leads to a purely elastic brittle behavior. On the contrary, it
A. B. Mosolov   +28 more
core   +1 more source

Analisa Kegagalan Blade Baris Terakhir Pada Rotor Turbine Uap Tipe Condensing [PDF]

open access: yes, 2014
Blades dari turbin uap merupakan komponen penting dalam pembangkit listrik. Analisa kegagalan blade turbin bertujuan untuk meningkatkan kehandalan sistem turbin secara umum. Kegagalan blade baris terakhir tekanan rendah yang terjadi pada turbine uap type
Komara, A. (Adhi), Kusuma, Y. (Yuriadi)
core   +2 more sources

Light and electron microscopy of microstructure and fractography of an ultrahigh-strength martensitic steel [PDF]

open access: yes, 2014
Microstructure, tensile properties and fractography have been examined in the oil-quenched samples of a low-alloy ultrahigh strength 4340 steel. Intergranular fracture was revealed to locate at the fracture origin.
Sha, Wei   +6 more
core  

Mechanical characteristics and failure analysis of AA6082/TiC/graphene hybrid composites

open access: yesMaterials Research Express
The main aim of the present research is to improve the tensile strength of lightweight aluminium alloy 6082, which makes it fit for many advanced engineering applications.
Sohan Lal   +4 more
doaj   +1 more source

Mechanism of strength degradation for hot corrosion of alpha-SiC [PDF]

open access: yes
Sintered alpha SiC was corroded by thin films of Na2SO4 and Na2CO3 molten salts at 1000%. This hot corrosion attack reduced room temperature strengths by as much as 50%.
Jacobson, N. S., Smialek, J. L.
core   +1 more source

Investigation of the Static and Dynamic Mechanical Properties of the Base Metal and Weld Zone of Haynes 25 Alloy [PDF]

open access: yesIranian Journal of Materials Science and Engineering
This work presents a comprehensive investigation of the high cycle fatigue behavior of Haynes 25 cobalt-based superalloy and its welds produced by pulsed continuous-wave (CW) laser welding.
Mahdi Behjati   +2 more
doaj  

Accelerated fatigue crack growth behavior of PWA 1480 single crystal alloy and its dependence on the deformation mode [PDF]

open access: yes
An investigation of the fatigue crack growth (FCG) behavior of PWA 1480 single crystal nickel base superalloy was conducted. Typical Paris region behavior was observed above a delta K of 8 MPa sq rt of m.
Ghosn, Louis J., Telesman, Jack
core   +1 more source

Calculation of Weibull strength parameters and Batdorf flow-density constants for volume- and surface-flaw-induced fracture in ceramics [PDF]

open access: yes
The calculation of shape and scale parameters of the two-parameter Weibull distribution is described using the least-squares analysis and maximum likelihood methods for volume- and surface-flaw-induced fracture in ceramics with complete and censored ...
Gyekenyesi, John P., Pai, Shantaram S.
core   +1 more source