Axial fully-reversed strain-controlled (R=−1) fatigue experiments were performed to obtain data demonstrating the effects of building orientation (i.e. vertical versus horizontal) and heat treatment on the fatigue behavior of 17–4 PH stainless steel (SS)
Aref Yadollahi +3 more
doaj +1 more source
The microstructure and mechanical properties of Al2214-8 wt.% of 500 nm sized B4C particles reinforced composites were studied in this study. By using a liquid metallurgical process, composites containing 8 wt.% of B4C in Al2214 alloy were created.
Gopalan Kumar +3 more
doaj +1 more source
A Guide to Forensic Fractography of Bone
The purpose of this guide is to familiarize the user with the science of fractography and how it can be used to examine and interpret skeletal fractures.
Angi M. Christensen +6 more
core +1 more source
The effect of platinum-aluminide coating features on high-temperature fatigue life of nickel-based superalloy Rene®80 [PDF]
Low cycle fatigue is the most important failure mode in Aviation/Industrial engine rotary turbine parts. In this paper, the influence of Pt-aluminide coating parameters on high temperature low cycle fatigue behavior of superalloy Rene®80 which is used to
Barjesteh M.M. +3 more
doaj +1 more source
Metal matrix nanocomposites (MMnCs) comprise a metal matrix filled with nanosized reinforcements with physical and mechanical properties that are very different from those of the matrix.
Aleksandar Vencl +5 more
doaj +1 more source
In the present research Al7075 alloy with 1, 3 and 5 varying weight percentages of flyash, 1, 2 and 3 varying wt.% of red mud along with constant 4 wt.% of mica particles composites were synthesized by stir casting technique.
Matti Siddesh +5 more
doaj +1 more source
Characterization of Corrosion and Stress Corrosion Cracking of AE44 Magnesium Alloy [PDF]
The paper presents the susceptibility of AE44 magnesium alloy to electrochemical corrosion and stress corrosion cracking (SCC). The evaluation of the intensity of the interaction of the corrosive environment was carried out using the corrosion tests and ...
M. Sozańska, A. Mościcki, B. Chmiela
doaj +1 more source
Effect of Dialkyl Peroxide Blending on Tensile Properties of PLA/PBAT Polymer Alloys
Poly(lactic acid) (PLA) and poly(butylene adipate/terephthalate) (PBAT) were used for polymer alloys, and the effects of the mixing ratio of PLA and PBAT and the addition of dialkyl peroxide (compatibilizing agent) were examined. The stress-strain curves
Masahiro NISHIDA +4 more
doaj +1 more source
Fractography of Bone Using Reconstructed Computed Tomography (CT) Scans: A Case Report Series
Fractography has been shown to be applicable to forensic assessments of skeletal trauma by observing the presence and orientation of fracture surface features, which reveal information about the direction of crack propagation.
Decker, Summer, Christensen, Angi
core +1 more source
The effect of microstructure on impact properties of AH80DBD low carbon bainite steel is analyzed by macro-fractography, scanning fractography, metallography and transmission electron microscope.