Results 41 to 50 of about 7,770 (217)
Herein, the stress corrosion cracking (SCC) susceptibility of duplex (UNS S32205) and austenitic (UNS S31653) stainless steel (SS) reinforcements was evaluated using integrity assessment criteria.
Ulises Martin, David M. Bastidas
doaj +1 more source
Fractography analysis of Inconel 718 fatigued at 700°C [PDF]
This work deals with the fractography analysis of nickel-base superalloy Inconel 718 fatigued at 700°C in air atmosphere in the high cycle region. During cyclic loading of this alloy at high temperatures some different mechanisms compared to cyclic ...
Otakar Bokůvka +7 more
core +1 more source
Fracture morphology of carbon fiber reinforced plastic composite laminates
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa +6 more
doaj +1 more source
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj +1 more source
Microstructural evolution of premium rail steel during flash butt welding (FBW), comparing physically simulated heat‐affected zones with actual weld regions. Thermal cycles induce phase transformations and microstructural heterogeneity that influence weld quality and mechanical performance. These findings provide insights into optimizing FBW parameters
Emmanoelle Cintra da Cunha Araújo +15 more
wiley +1 more source
Fractography is the study of fracture surface morphology, and it can be used to assess a material’s mechanical properties as well as to determine the underlying mechanisms leading to material failure.
Maureen Bottrell +11 more
core +1 more source
The present work reports the microstructural, mechanical, and texture evolution of a dissimilar combination laser‐welded maraging steel with 4340 steel. This is important for aerospace applications. The demand for dissimilar welding is growing rapidly with the requirement of efficient and durable joints.
Bharat Behl +3 more
wiley +1 more source
As the first major reference on glass fractography, contributors to this volume offer a comprehensive account of the fracture of glass as well as various fracture surface topography Contributors discuss optical fibers, glass containers, and flatglass ...
Tressler, Richard, Bradt, Richard
core +1 more source
Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen +16 more
wiley +1 more source
Study of fractography of ferritic ductile iron at different temperatures and loading conditions
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang +9 more
doaj +1 more source