Fractography of ice

Journal of Materials Science Letters, 1989
Etude experimentale par microscopie electronique analytique. La rupture de la glace a grains fins entre −25 et −50C est une rupture transgranulaire par clivage.
E. M. Schulson   +4 more
openaire   +1 more source

Fractographie - Bases physiques

Étude et propriétés des métaux, 2002
Un organe mecanique est un element destine au fonctionnement d’un ensemble machine ou d’une structure metallique, chaque element ayant une fonction determinee, en parallele ou en serie, avec d’autres organes. Sa conception entraine sa fabrication : elaboration du materiau, transformation (mise en forme a chaud ou a froid), traitement en volume ou en ...
Annick POKORNY, Jean POKORNY
openaire   +1 more source

Mechanical Fractography and Worn Surface Analysis of Nanographite and ZrO2-Reinforced Al7075 Alloy Aerospace Metal Composites

Journal of Failure Analysis and Prevention, 2021
Raj Kumar   +5 more
semanticscholar   +1 more source

Fractography

Volume 12 covers all aspects of fractography relevant to its use in materials evaluation, failure analysis, and quality control. In addition to an extensive collection of fractographs, it includes information on the types and appearances of fracture, visual examination and imaging methods, quantitative fractography, surface profiling, and fractal ...
openaire   +1 more source

Electron Fractography

1968
Description The Symposium on Electron Fractography was presented during the Seventieth Annual Meeting of the Society held in Boston, Mass., 25—30 June 1967. The symposium was sponsored by Committee E24 on Fracture Testing of Metals. The symposium chairman was C. D. Beachem, Naval Research Laboratory.
openaire   +1 more source

Fractals in fractography

Materials Science and Engineering, 1986
Abstract The fractal characteristics of a series of fractured AISI 4340 steel specimens were studied experimentally by means of vertical sections through the fracture surface. Extensive fractal data have been generated for both the fracture surfaces and their profiles.
Ervin E Underwood, Kingshuk Banerji
openaire   +1 more source

Fractography of Weldments

Abstract This article provides an overview of fractography as it applies to metal weldments and presents examples of various fracture surface morphologies to demonstrate how fractographic analysis can be used to determine the cause of weld failures.
J.R. Stewart   +4 more
openaire   +1 more source

Fractography of Fiberglass

1994
This paper discusses the applications and the limitations of the fractography technique as applied to the fiberglass industry. The main limitation of fractography originates from the fact that fibers of strength greater than about 2000 MPa shatter into multiple small fragments upon fracture rendering it impossible to capture the true fracture surfaces.
openaire   +1 more source

Fractography of Polymers

Abstract This article provides an overview of polymer fractography, with examples of various fracture surfaces created under diverse loading conditions. The focus is on the interpretation of polymer fracture-surface features in light of the unique viscoelastic nature of polymers.
Jericho Moll, Corissa Lee
openaire   +1 more source