Materials Science and Engineering, 1986
Abstract The fractal characteristics of a series of fractured AISI 4340 steel specimens were studied experimentally by means of vertical sections through the fracture surface. Extensive fractal data have been generated for both the fracture surfaces and their profiles.
Ervin E Underwood, Kingshuk Banerji
openaire +1 more source
Abstract The fractal characteristics of a series of fractured AISI 4340 steel specimens were studied experimentally by means of vertical sections through the fracture surface. Extensive fractal data have been generated for both the fracture surfaces and their profiles.
Ervin E Underwood, Kingshuk Banerji
openaire +1 more source
Fractography of Metals and Plastics
Practical Failure Analysis, 2001Fractography is critical to failure analysis of metals and plastics. Fractography of plastics is a relatively new field with many similarities to metals. Using case histories, various aspects of failure analysis and fractography of metals and plastics are compared and contrasted. Failure modes common to both metals and plastics include ductile overload,
openaire +1 more source
Materials Today: Proceedings, 2019
Laser additive manufacturing (LAM) is the process used to fabricate near net shape from metallic powders. A major challenge with LAM fabricated parts is the materials performance to achieve required mechanical properties.
Tarun Bhardwaj, M. Shukla
semanticscholar +1 more source
Laser additive manufacturing (LAM) is the process used to fabricate near net shape from metallic powders. A major challenge with LAM fabricated parts is the materials performance to achieve required mechanical properties.
Tarun Bhardwaj, M. Shukla
semanticscholar +1 more source
Additive Manufacturing, 2019
To reduce the lead time, polymer fuel tanks could be toollessly produced using additive manufacturing (AM) technologies. Detailed knowledge of the performance of AM polymers is essential for the design and development of such components.
David Tasch +3 more
semanticscholar +1 more source
To reduce the lead time, polymer fuel tanks could be toollessly produced using additive manufacturing (AM) technologies. Detailed knowledge of the performance of AM polymers is essential for the design and development of such components.
David Tasch +3 more
semanticscholar +1 more source
2001
Abstract This article illustrates typical fractographic features for a number of different composite materials. It describes the differences in fracture characteristics due to different loading, material processing, and environmental conditions. The article presents fractographic data obtained from epoxy matrix materials.
openaire +1 more source
Abstract This article illustrates typical fractographic features for a number of different composite materials. It describes the differences in fracture characteristics due to different loading, material processing, and environmental conditions. The article presents fractographic data obtained from epoxy matrix materials.
openaire +1 more source
IEEE transactions on dielectrics and electrical insulation, 2018
A field brittle fracture composite insulator was examined and analyzed in detail in terms of chemical property and fractography with the purpose of obtaining the cause and mechanism of the failure as well as providing more detailed information on acid ...
Yan-Feng Gao +4 more
semanticscholar +1 more source
A field brittle fracture composite insulator was examined and analyzed in detail in terms of chemical property and fractography with the purpose of obtaining the cause and mechanism of the failure as well as providing more detailed information on acid ...
Yan-Feng Gao +4 more
semanticscholar +1 more source
Journal of Materials Science Letters, 1989
Etude experimentale par microscopie electronique analytique. La rupture de la glace a grains fins entre −25 et −50C est une rupture transgranulaire par clivage.
E. M. Schulson +4 more
openaire +1 more source
Etude experimentale par microscopie electronique analytique. La rupture de la glace a grains fins entre −25 et −50C est une rupture transgranulaire par clivage.
E. M. Schulson +4 more
openaire +1 more source
Journal of the Geological Society, 1994
The first thematic meeting on fractography in geology, held on 13 September at Burlington House, London, was jointly sponsored by the Petroleum Group and the Tectonic Studies Group of the Geological Society. It was attended by 50 participants from Australia, Canada, France, Germany, Holland, Norway, Sweden, United Kingdom and the United States of ...
openaire +1 more source
The first thematic meeting on fractography in geology, held on 13 September at Burlington House, London, was jointly sponsored by the Petroleum Group and the Tectonic Studies Group of the Geological Society. It was attended by 50 participants from Australia, Canada, France, Germany, Holland, Norway, Sweden, United Kingdom and the United States of ...
openaire +1 more source
Quantitative fractography for brittle fracture via multilayer perceptron neural network
Engineering Fracture Mechanics, 2023A. Jafari +3 more
semanticscholar +1 more source
Abstract This article provides an overview of fractography as it applies to metal weldments and presents examples of various fracture surface morphologies to demonstrate how fractographic analysis can be used to determine the cause of weld failures.