Results 21 to 30 of about 2,431 (185)

Effects of hydrogen gas pressure and test frequency on fatigue crack growth properties of low carbon steel in 0.1-90 MPa hydrogen gas

open access: yesNihon Kikai Gakkai ronbunshu, 2014
In order to investigate the effects of hydrogen gas pressure pH2 and test frequency f on the fatigue crack growth (FCG) properties of low carbon steel in hydrogen gas atmosphere, the FCG tests using compact tension specimens were conducted under various ...
Michio YOSHIKAWA   +4 more
doaj   +1 more source

Off-Axis Tension Behaviour of Unidirectional PEEK/AS4 Thermoplastic Composites

open access: yesApplied Sciences, 2023
An experimental method for non-standard off-axis tension tests of unidirectional composites is developed. A new oblique end-tab is designed to eliminate stress concentration and in-plane bending moment induced by off-axis tension loading.
Yifan Ma, Yazhi Li, Lu Liu
doaj   +1 more source

Fatigue Behavior of an Al-12.7Si-0.7Mg Alloy Processed by Extrusion and Heat Treatment

open access: yesFrontiers in Materials, 2021
The fatigue life of a hot extruded Al-12.7Si-0.7Mg alloy under T1, T4, and T6 conditions was studied. The microstructure and tensile properties of the alloy were investigated in order to analyze the fatigue behavior.
Fang Liu, Fuxiao Yu, Dazhi Zhao, Li Gao
doaj   +1 more source

Effect of Hydrogen Content and Strain Rate on Hydrogen-induced Delay Cracking for Hot-stamped Steel

open access: yesMetals, 2019
Hot-stamped steel has been widely used in automobile bumper and other safety components due to its high strength. Therefore, this paper investigates the effect of hydrogen content and strain rate on hydrogen-induced delay cracking (HIDC) behavior.
Hongxing Jia   +4 more
doaj   +1 more source

The Combined Effect of Banana Fiber and Fly Ash Reinforcements on the Mechanical Behavior of Polyester Composites

open access: yesJournal of Natural Fibers, 2022
The mechanical behavior of banana fiber (BA) reinforced polymer composites filled with fly ash (FA) is analyzed in this present investigation. Polyester matrix is used to produce composites with 30% of banana fiber volume and fly ash with three separate ...
Gokul Kannan   +3 more
doaj   +1 more source

Integrity Assessment of Stress Corrosion Cracking Susceptibility of Duplex UNS S32205 and Austenitic UNS S31653 Stainless Steel Reinforcements

open access: yesMetals, 2023
Herein, the stress corrosion cracking (SCC) susceptibility of duplex (UNS S32205) and austenitic (UNS S31653) stainless steel (SS) reinforcements was evaluated using integrity assessment criteria.
Ulises Martin, David M. Bastidas
doaj   +1 more source

Fracture morphology of carbon fiber reinforced plastic composite laminates

open access: yesMaterials Research, 2010
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa   +6 more
doaj   +1 more source

Experimental investigation of shape memory polymer hybrid nanocomposites modified by carbon fiber reinforced multi-walled carbon nanotube (MWCNT)

open access: yesMaterials Research Express, 2021
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj   +1 more source

Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite

open access: yesAdvanced Functional Materials, EarlyView.
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen   +16 more
wiley   +1 more source

Unique Role of Microstructure of a Bioimplant Zinc Alloy and Protein Content of Simulated Body Fluid in Corrosion and Fracture

open access: yesAdvanced Functional Materials, EarlyView.
BSA addition to physiological solutions enhances resistance of a Zn alloy to stress corrosion cracking (SCC) but reduces its corrosion resistance. Extended surface characterization explains the contrasting influences on corrosion and SCC. Unexpectedly, the alloy suffers transgranular SCC (TGSCC), despite extensive grain boundary precipitation. Thorough
RK Singh Raman   +9 more
wiley   +1 more source