Results 31 to 40 of about 2,431 (185)
To address functionality limitations in plant‐based and industrially compostable polymer aerogels, this work introduces bio‐inspired aerogels with broadened functionality. Inspired by functional plant tissues, lightweight biopolymer aerogels based on exclusively stereocomplex crystals are fabricated, featuring hierarchically macro‐/meso‐porous ...
Anthony V. Tuccitto +10 more
wiley +1 more source
Study of fractography of ferritic ductile iron at different temperatures and loading conditions
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang +9 more
doaj +1 more source
Green mechanochemical copolymerization was developed for universal interfacial modification of Group 13 and related fillers. By leveraging Lewis acid–base coordination to anchor sulfur‐containing polymers—validated via multiscale characterization and DFT—this versatile method boosts performance across liquid fuels, thermal‐shielding materials, and ...
Chen Wang +7 more
wiley +1 more source
From Posidonia oceanica seagrass fibers to sustainable bio‐composites: the role of alkaline treatment in composite performance and durability. ABSTRACT The valorization of the abundant marine residue Posidonia oceanica (PO) fibers, as a filler in a bio‐based epoxy matrix was investigated.
Mahamat Saleh Elhadj Yacoub +4 more
wiley +1 more source
Microscopic observation of creep-fatigue crack propagation in lead-free solder
Creep-fatigue crack propagation tests of lead-free solder were conducted under various loading waveforms. The waveforms adapted in displacement-controlled tests were four triangular waveforms: pp waveform having fast loading-unloading, cc waveform having
Keisuke TANAKA +4 more
doaj +1 more source
Tufting‐Based Manufacturing Method for High‐Performance 3D Composite Lap Joints
Graphical abstract illustrating the manufacturing process of a tufted non‐crimp preform lap joint, fractographic characterisation and comparative mechanical performance evaluation. ABSTRACT This study presents a tufting‐enabled through‐thickness reinforcement approach for enhancing the performance of 3D composite lap joints manufactured using resin ...
J. Ahmed +3 more
wiley +1 more source
Effect of Temperature on Tensile Properties of Electrospun Nanofibre Interleaved Carbon Composites
Thermal Durability of Electrospun Nanofibre Interleaved Composites. ABSTRACT Carbon fiber composites are susceptible to brittle damage modes such as matrix cracking and delamination. The inception and propagation of these invisible damages are responsible for loss in load‐bearing capacity and accelerating environmental degradation.
Usaid Ahmed Shakil +5 more
wiley +1 more source
Overview of the study evaluating the impact of post‐print annealing on the microstructural crystallization and thermomechanical properties of FDM‐printed high‐temperature PLA and glass fiber‐reinforced PLA composites. ABSTRACT Polylactic acid (PLA) combines renewable sourcing and reliable printability with limited stiffness retention near its glass ...
Huseyin Erdem Yalkin, Ayse Nur Ozkan
wiley +1 more source
Ultrasonic fracturing (UF) can be used to form crack networks for oil or gas in the mining industry and hard rock excavation. In this paper, the three-dimensional internal laser-engraved crack method (3D-ILC) is introduced to make penny-shaped internal ...
Haijun Wang +4 more
doaj +1 more source
The multi‐scale mechanical behavior of additive‐manufactured 316L stainless steel processed by directed energy deposition and high‐pressure torsion is explored. The influence of torsional strain on strength and microstructural evolution is revealed, indicating progressive grain refinement in the ultrafine regime, reaching strength levels nearing 1800 ...
M. Farhan Raza, Guney Guven Yapici
wiley +1 more source