Results 201 to 210 of about 162,548 (258)
A porous parylene‐coated electrode loaded with dexamethasone was developed to reduce inflammation after cochlear implantation. In guinea pigs, the device provided sustained drug release, maintained biocompatibility, improved auditory brainstem response thresholds, and reduced inflammatory cell infiltration and TNF‐α expression.
Chi‐Chieh Chang +11 more
wiley +1 more source
Multifunctional Y<sub>2</sub>O<sub>3</sub>-Modified Borotellurite Bioactive Glasses for Bone Tissue Engineering Applications. [PDF]
Oruc Ulas E +6 more
europepmc +1 more source
Structural Origins of High MoO<sub>3</sub> Solubility in Peraluminous Borosilicate Glasses. [PDF]
Joseph NDI +6 more
europepmc +1 more source
NovaBone Bioactive Glass for Oral Bone Regeneration: Mechanisms, Innovations, and Clinical Outcomes. [PDF]
Khan MA +7 more
europepmc +1 more source
Diatomite from West Kazakhstan as a Sustainable Raw Material for Borosilicate Glass Production. [PDF]
Satayeva S +4 more
europepmc +1 more source
Evaluation of the Sealing Ability and Penetration Depth of the TheraCal LC as a Sealant for Pit and Fissures: An <i>In Vitro</i> Study. [PDF]
Eddula RR +3 more
europepmc +1 more source
Some of the next articles are maybe not open access.
Related searches:
Related searches:
The effect of Y on glass forming ability
Scripta Materialia, 2005Abstract We have discovered a new glass forming region (GFR) defined by melt-spinning at a speed of 30 m/s in a ternary Fe–Fe2B–Fe4B4Y eutectic in the Fe–B–Y alloy system. This GFR is remarkably wide, within the compositional range 19–40 at.% B, 3 to ∼10 at.% Y and 76–50 at.% Fe, with the best glass former being Fe71.2B24Y4.8 for a 1 mm fully ...
Yi Li, Y P Feng
exaly +2 more sources
Glass forming ability of bulk glass forming alloys
Scripta Materialia, 1997In general, rapid quenching from the melt at cooling rates in the range of 10{sup 4} to 10{sup 6} K/s is required to obtain glass formation in metallic alloys. However, recent development have shown that bulk glass formation at cooling rates as low as {approximately}1 K/s can also be obtained in Zr, Mg, La, Nd, Ti, Cu and Fe based metallic alloy ...
Li, Y. +4 more
openaire +1 more source
Glass-forming ability of alloys
Journal of Non-Crystalline Solids, 1993Abstract New amorphous alloys exhibiting a wide supercooled liquid region before crystallization were found to form by melt spinning in wide composition ranges of LaAlM, MgYM and ZrAlM (M = Ni or Cu) systems consisting of the constituent elements with significantly different atomic sizes.
Akihisa Inoue +2 more
openaire +1 more source