Results 1 to 10 of about 70,065 (127)

Hot Ductility Loss in a Fe-Ni-Based Superalloy [PDF]

open access: yesMetals, 2015
High temperature tensile tests have been conducted on samples of a Fe-Ni based superalloy, Incoloy A-286, and significant ductility loss has been observed at 1220 °C.
Chen-Wei Li   +3 more
doaj   +5 more sources

Hot Ductility Loss and Recovery in the CGHAZ of T23 Steel during Post-weld Heat Treatment at 750°C

open access: yesISIJ International, 2017
T23 is used at 500 to 600°C in modern power station. The chemical composition is designed with respect for manufacture of membrane walls without preheating and, if possible, without heat treatment.1) The weldability is improved by decreasing carbon ...
Jin, Yujing, Zhou, Wei
exaly   +4 more sources

The Relationship between Tensile Ductility Loss and Microstructures for the Hot Exposed γ-Tial Alloys

open access: yesAdvanced Materials Research, 2012
In this paper, the relationship between the tensile ductility loss and the conditions including the exposure process and microstructures for the hot exposed TiAl alloys was researched. The critical temperature corresponding to the ambient tensile ductility loss to 0.8% was sensitive to the microstructure.
Xiao Hong Li, Li Xiao Hong
exaly   +5 more sources

The Mechanism of Hot Ductility Loss and Recovery in Nb-Bearing Low Alloy Steels [PDF]

open access: yesMetallurgical and Materials Transactions A, 2014
In low alloy steels containing Nb, the poor hot ductility is basically due to the austenite grain boundary segregation of sulfur and the additional matrix strengthening of Nb(C,N) precipitates, both of which decrease the equicohesive temperature. The recovery of hot ductility is therefore attributed to not only the clean grain boundaries that the ...
Myeong Hun Kang   +4 more
openaire   +3 more sources

Hot Ductility of TiNb IF Steel Slab after Hot Torsion Testing

open access: yesMetals, 2019
The aim of the work was to evaluate the hot ductility loss in TiNb stabilized IF steel directly from the continuously-cast slab using hot torsion testing (plastometry) in the temperature range 600−1250 °C according to the basic programme, and ...
Jana Konrádyová   +10 more
doaj   +2 more sources

Hot ductility behavior of new Ni-based superalloy G27: Influence of solution annealing on the liquation cracking susceptibility

open access: yesJournal of Materials Research and Technology
The hot ductility behavior of new Ni-based superalloy G27 was investigated using Gleeble™ 3800 under various standard solution-annealing conditions to study how solution annealing treatments, which result in different grain sizes, affect the alloy's ...
Achmad Ariaseta   +3 more
doaj   +2 more sources

Mechanism for Loss of Hot Ductility Due to Deformation during Solidification in Continuous Casting of Steel

open access: yesISIJ International, 2004
Strand surface cracking is a problem that can lead to scrap the product of the continuous casting process. Stress and strain developed during continuous casting have been found to be effective in this respect. The crack susceptibility is usually evaluated by assessing the steel hot ductility at the straightening stage of the process.
Zarandi, Faramarz, Yue, Steve
openaire   +3 more sources

Hot ductility behavior of AD730™ nickel-base superalloy

open access: yesMaterials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing, 2019
Hot ductility of the newly developed AD730™ nickel-base superalloy was investigated in the temperature interval 1050–1240 °C. The nil strength and nil ductility temperatures were determined by hot tensile testing using the Gleeble™ 3800 weld thermal ...
Seyedmohammad Tabaie   +2 more
exaly   +2 more sources

Effect of Solution Temperature on the Microstructure and Properties of AlSi37Cu0.7Mg0.9Ni0.2 Alloy Prepared by Rapid Solidification and Hot Extrusion. [PDF]

open access: yesMaterials (Basel)
This study systematically investigated the effects of solution temperature (460–560 °C) on the microstructure, mechanical properties, and corrosion behavior of AlSi37Cu0.7Mg0.9Ni0.2 alloy rods prepared by rapid solidification and hot-extrusion.
Mao X, Chen Z, Gu N, Huang D, Zhuang L.
europepmc   +2 more sources

Increasing the ductility of the Al-Si alloy with low silicon content by deformation-heat treatment [PDF]

open access: yesМеталознавство та обробка металів, 2021
A method of deformation-heat treatment is considered for Al-Si alloy with 4.5 % silicon, which consists in a series of small hot deformations with intermediate annealing.
V.V. Kaverinsky   +3 more
doaj   +1 more source