Results 51 to 60 of about 5,447 (260)
Effect of Ti Addition on the Hot-Tearing Susceptibility of the AlSi5Cu2Mg Alloy
The aluminum alloy AlSi5Cu2Mg finds application in the production of high-stress cylinder head castings. The AlSi5Cu2Mg alloy is specific for its high susceptibility to hot tearing.
Marek Matejka +2 more
doaj +1 more source
Effect of die coating on surface crack depth of hot extruded 7075 aluminum alloy
The aluminum alloys belonging to the 7000 series are high-strength alloys used in a wide variety of products for weight reduction. They are primarily used in the field of transportation and aerospace. Among these, the A7075 alloy has the highest strength
Tatsuya Funazuka +4 more
doaj +1 more source
This review comprehensively evaluates extrusion‐based additive manufacturing for advanced ceramics, detailing feedstock options and key process parameters. By critically addressing defect mechanisms like porosity and cracking, the work highlights optimization strategies through machine learning and advanced postprocessing.
Meisam Bakhtiari +4 more
wiley +1 more source
Formation of Hot Tear Under Controlled Solidification Conditions [PDF]
Aluminum alloy 7050 is known for its superior mechanical properties, and thus finds its application in aerospace industry. Vertical direct-chill (DC) casting process is typically employed for producing such an alloy. Despite its advantages, AA7050 is considered as a “hard-to-cast” alloy because of its propensity to cold cracking.
Subroto, T +8 more
openaire +3 more sources
Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi +5 more
wiley +1 more source
Influence of Ni content on hot tearing tendency of Al-5.6Zn-2.5Mg-1.6Cu alloys
A combination of numerical simulation and experimental methods was used to study the influence of Ni content on the hot tearing tendency of Al-5.6Zn-2.5Mg-1.6Cu-xNi (x=0%,0.1%,0.3%,0.5%,mass fraction, the same below) alloys.
XIA Can +6 more
doaj +1 more source
Controlling the Field Assisted Sintering Technology (FAST) parameters, dwell temperature and cooling rate, significantly influences the microstructural evolution in titanium aluminide GE4822. Significant γ‐lamellar colonies develop only upon cooling through the α‐transus.
Jack Krohn, James Pepper, Martin Jackson
wiley +1 more source
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees +6 more
wiley +1 more source
Hot tearing behavior and mechanism of AXJ530 alloy under rotating magnetic field
In order to solve the issues concerning high hot tearing susceptibility (HTS) of Mg-Al-Ca series alloys, a rotating magnetic field (RMF) was applied during their solidification.
Xudong Du +7 more
doaj +1 more source
Hot tearing susceptibility (HTS) of Mg–2Zn–(3 + 0.5x)Y–xAl (x = 0, 2 and 3 at%) alloys is predicted by using modified Clyne–Davies’ model (CSC*). The solidification path, solidification characteristic temperatures and dendritic coherency solid fraction ...
Guojia Zhang +3 more
doaj +1 more source