Results 51 to 60 of about 1,171,203 (263)
Hot tearing in aluminium-copper alloys
For many aluminium alloys, hot tearing susceptibility follows a lambda curve relationship when hot tearing severity is plotted as a function of solute content. In the past, there has been some difficulty quantifying hot tearing.
David StJohn +7 more
core +1 more source
In Situ Magnetic Ordering and Microfabrication of Liquid Crystal Networks with Discretized Alignment
Miniaturizing liquid crystal network actuators typically demands costly laser writing or digital light processing. A low‐cost photolithography platform couples rotating photomasks with a Halbach magnetic array to discretize in‐plane molecular alignment down to 50 µm, producing programmable, light‐responsive grippers, checkerboards, and origami‐inspired
Matthew Gene Scarfo +3 more
wiley +1 more source
The hot tearing of 6xxx-series aluminium alloys has been investigated over four levels of silicon (0.6, 0.8, 1.0, 1.2 wt%), magnesium (0.4, 0.6, 0.8, 1.0 wt%), iron (0.2, 0.4, 0.6, 0.8 wt%) and manganese (0.0, 0.2, 0.4, 0.6 wt%).
Emidio Giansante +3 more
doaj +1 more source
Nitride MXenes remain constrained by a persistent gap between computational prediction and experimental realization. This Review identifies the thermodynamic, kinetic, and chemical barriers limiting their synthesis, critically evaluates emerging fabrication routes, and proposes a multidimensional computational‐experimental framework to accelerate the ...
Naresh Varnakavi, Masoud Soroush
wiley +1 more source
Biodegradable 3D‐Printable and Coatable Antifouling Composites for Marine Applications
Marine biofouling damages submerged surfaces and raises greenhouse gas emissions. Biodegradable antifouling biocomposites were developed by hot‐mixing beeswax, Tween 80, and calcium stearate or stearic acid. Adjusting the component ratio enables processing via hot‐pressing, 3D‐printing, or dip‐coating.
Gabriele Corigliano +17 more
wiley +1 more source
Influences of Y Additions on the Hot Tearing Susceptibility of Mg-1.5wt.%Zn Alloys [PDF]
The influences of Y (0.2, 2 and 4 wt.%) additions on the hot tearing behaviour of Mg‑1.5Zn alloys were investigated using a constrained rod casting (CRC) apparatus equipped with a load cell and data acquisition system. The initiation of hot tearing was monitored during CRC experiments. It corresponds to a drop in load on the hot tearing curves.
Wang, Z. +5 more
openaire +2 more sources
Bioinspired Adaptive Sensors: A Review on Current Developments in Theory and Application
This review comprehensively summarizes the recent progress in the design and fabrication of sensory‐adaptation‐inspired devices and highlights their valuable applications in electronic skin, wearable electronics, and machine vision. The existing challenges and future directions are addressed in aspects such as device performance optimization ...
Guodong Gong +12 more
wiley +1 more source
Lignin‐mimicking protein methylation can enhance the efficacy and mitigate the toxicity of the classic FOLFOX chemotherapy regimen. ABSTRACT FOLFOX has served as the standard chemotherapy regimen for advanced stages, specifically in the treatment of pancreatic, colorectal, and bladder cancers.
Shiyao Song +14 more
wiley +1 more source
The brittle behaviour of Fe/Al intermetallic compounds formed during dissimilar Al-to-steel welding is a major drawback for the mechanical integrity of the joint, particularly for thick intermetallic layers. In order to improve the toughness of the weld,
N. Jimenez-Mena, A. Simar, P.J. Jacques
doaj +1 more source
A circular upcycling strategy transforms waste poly(ethylene terephthalate) bottles into microwave‐responsive Ni@C catalyst featuring lattice‐distorted nickel cores and defective carbon shells. These strain‐rich heterointerfaces enhance dielectric loss and promote localized microwave hotspots, accelerating peroxymonosulfate activation and polymer‐chain
Xiao Lu +7 more
wiley +1 more source