Microstructural evolution of Mn-based maraging steels and their influences on mechanical properties [PDF]
The microstructural evolution in a set of Mn-based maraging steels (7–12 wt% Mn) when aged at 460–500 ºC for various durations up to 10,080 min and the influences on mechanical properties are systematically investigated.
Qian, F., Rainforth, W.M., Sharp, J.
core +1 more source
Improving Toughness of PH13-8 Stainless Steel through Intercritical Annealing
An intercritical annealing step was introduced in the treatment of a PH13-8 stainless steel to improve the toughness of the alloy in aged condition. Four different treatment cycles, i.e. austenitisation (Q-treatment) and intercritical anneal (L-treatment), LQ, 2B (QLQL) and 2K (LQLQ) were carried out before aging treatment at 510°C for 4 h (the ...
Guo, Z. +3 more
openaire +2 more sources
Fe–12Mn–0.2C medium‐manganese steel is processed by laser‐based powder bed fusion of metals using blended as well as pre‐alloyed powder. Various scanning speeds are used to determine the influence of energy deposition rate on microstructure and mechanical properties.
Leoni Hübner +4 more
wiley +1 more source
In this study, we used 0.2C-1.7Si-1.9Mn wt% cold-rolled sheet as the experimental material to prepare the Q&P sample with blocky microstructures and the QQ&P sample with lath-shaped microstructures through the Q&P and QQ&P processes, respectively.
Huan Xiao +4 more
doaj +1 more source
Mechanical Properties Improvement of Low Carbon Steel by Combined Heat Treatments [PDF]
The improvement of the Mechanical properties of the low Carbon steel and increasing its strength, was the goal of some heat treatment technologies developed in the last twenty years. One of these technologies is the Rapid Heat Treatment (RHT), by which
Abou-Jahjah, J., Dobránszky, János
core
Heat treatment parameters critically affect the wear resistance of powder bed fusion–laser beam (PBF‐LB)‐produced Ti–6Al–2Sn–4Zr–6Mo alloy. This study found that optimizing annealing temperature allows to obtain a tailored microstructure, which enhances the dry‐sliding behavior by forming a stable and functional mechanically mixed layer (MML), ensuring
Gianluca Pirro +5 more
wiley +1 more source
The influence of starting point microstructures on the transformation mechanisms and mechanical properties of a micro alloyed steel after annealing in the alpha + gamma region have been investigated.
Ovri Henry, Kamma Celestine Monde
doaj +1 more source
A new austempering approach following intercritical austenitizing is explored to improve the mechanical behavior of API 5CT steel. By tailoring ferrite–bainite microstructures, the process achieves a balance of strength and ductility without the need for post‐quench tempering. The results highlight a cost‐effective alternative to conventional quenching
Paulo Henrique Cirilo +2 more
wiley +1 more source
Comparison of Heat Treatments on the Toughness of 1.7Ni-1.5Cu-0.5Mo Pre-alloyed P/M Steels
Effects of quenching plus tempering and intercritical annealing plus quenching heat treatments on the impact toughness properties of 1.7Ni-1.5Cu-0.5Mo pre-alloyed powder metallurgy steels with 0.2 (in mass%) graphite were investigated.
Güral Ahmet, Türkan Mustafa
doaj +1 more source
Thermomechanical Processing, Microstructure, and Mechanical Properties of Medium‐Mn Steel
The microstructure evolution and mechanical properties of a medium‐Mn steel are investigated after thermomechanical processing and isothermal holding at various temperatures. A fine multiphase structure of bainite, fresh or tempered martensite, and retained austenite are obtained.
Burak Barutçuoğlu +3 more
wiley +1 more source