Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales

open access: yesAdvanced Engineering Materials, EarlyView.
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik   +7 more
wiley   +1 more source

Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A

open access: yesAdvanced Engineering Materials, EarlyView.
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han   +5 more
wiley   +1 more source

Iron Restriction [PDF]

open access: yesEvolution, Medicine, and Public Health, 2015
openaire   +2 more sources

High‐Temperature Nanoindentation of Metals: Assessing Thermal Drift, Frame Compliance, and Chemical Composition Effects on the Reported Mechanical Properties

open access: yesAdvanced Engineering Materials, EarlyView.
Do not let thermal drift and instrument artifacts deceive high‐temperature nanoindentation results. We compare classical Oliver–Pharr and automatic image recognition analyses across steels and a Ni alloy to quantify these effects. Accounting for artifacts reveals systematic softening with temperature, while Cr and Ni additions boost resistance ...
Velislava Yonkova   +2 more
wiley   +1 more source

Recycling of NiTi Shape Memory Alloys: Fundamental and Technological Aspects of a Vacuum Induction Melting Processing Route

open access: yesAdvanced Engineering Materials, EarlyView.
The present study investigates recycling of NiTi shape memory alloys via vacuum induction melting. An ingot was synthesized from elemental Ni and Ti and subjected to three subsequent remelting cycles. Remelting increases process durations and impurity levels and adversely affects microstructures and functional properties.
Sakia Sophia Noorzayee   +7 more
wiley   +1 more source

Direct Metal Deposition of Graphene–Ti28Nb35.4Zr Matrix Composites With Enhanced Mechanical, Corrosion, and Biocompatibility Properties for Bone Implants

open access: yesAdvanced Engineering Materials, EarlyView.
Graphene nanoplatelet (0.1 wt.%) reinforcement significantly enhances the performance of β Ti‐28Nb‐35.4Zr alloy. Grain refinement, reduced water contact angle, and improved surface characteristics promote osteoblast adhesion and complete surface coverage after 7 days.
Khurram Munir   +5 more
wiley   +1 more source

Toward Knowledge‐Based Workflows: A Semantic Approach to Atomistic Simulations for Mechanical and Thermodynamic Properties

open access: yesAdvanced Engineering Materials, EarlyView.
Knowledge‐based atomistic workflows are presented for mechanical and thermodynamic properties. By coupling modular simulations with ontology‐aligned metadata and provenance, Fe case studies on elastic behavior, defects, thermal properties, and Hall–Petch strengthening reveal how FAIR, queryable, and reusable simulation data can be generated. Mechanical
Abril Azócar Guzmán   +5 more
wiley   +1 more source

Home - About - Disclaimer - Privacy