Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
Geometry‐driven thermal behavior in wire‐arc additive manufacturing (WAAM) influences microstructural evolution during nonequilibrium solidification of a chemically complex Fe–Cr–Nb–W–Mo–C nanocomposite system. By comparing different deposits configurations, distinct entropy–cooling rate correlations, segregation, and carbide evolution are revealed ...
Blanca Palacios +5 more
wiley +1 more source
Improvement of the stoping technology in mining magnetite quartzite by underground methods [PDF]
The ore deposits in Kryvyi Rih iron ore basin are mined using bulk ore and overlying rocks caving systems. These mining systems have a significant drawback, namely a 2 – 5% reduction in the iron content of the mined ore mass when mining rich ores and up ...
Pysmennyi Serhii +5 more
doaj +1 more source
Towards Defect Phase Diagrams: From Research Data Management to Automated Workflows
A research data management infrastructure is presented for the systematic integration of heterogeneous experimental and simulation data required for defect phase diagrams. The approach combines openBIS with a companion application for large‐object storage, automated metadata extraction, provenance tracking and federated data access, thereby supporting ...
Khalil Rejiba +5 more
wiley +1 more source
Karl Popper and the Mechanisms of Hydrogen Embrittlement
Representation of the beginning of loss of ductility rather than embrittlement. Small concentrations of hydrogen in a diffusible form within iron are well‐established to harm the mechanical integrity of steels. There are theories that attempt to explain the pernicious role of hydrogen.
H. K. D. H. Bhadeshia
wiley +1 more source
PWM inverter-excited iron loss characteristics of a reactor core
In this paper, we focus on an evaluation of iron losses in a reactor core under pulse width modulation (PWM) inverter excitation. We examine the inverter- and sinusoidal-fed iron losses of the reactor core through both experiments and numerical ...
Atsushi Yao +6 more
doaj +1 more source
AC Iron Loss Prediction and Magnetic Properties of Fe-6.5 wt. % Si Ribbons Prepared by Melt-Spinning
Ultra-thin Fe-6.5 wt. % Si ribbons of 35 μm in thickness were prepared by melt-spinning. The magnetic properties were investigated before and after annealing at 1000 °C.
Shuai Wang +4 more
doaj +1 more source
Equivalent magnetic circuit method of estimating iron losses in induction motor spindles. [PDF]
Lü L, Xiong W, Hu C.
europepmc +1 more source
Identified through the use of statistical design of experiments and metallographic investigation, this study exposes the stochastic origins of intergranular cracks in blown powder laser beam directed energy deposition additive manufacturing of pure molybdenum. It further demonstrates a successful crack mitigation approach with direct correlation to the
Nathaniel J. Lies +2 more
wiley +1 more source
Calculated versus measured iron losses and instantaneous magnetization power functions of electrical steel. [PDF]
Pfützner H, Shilyashki G, Huber E.