Microstructure Evolution of a VMnFeCoNi High‐Entropy Alloy After Synthesis, Swaging, and Annealing
The synthesis and processing (rotary swaging and annealing) of the novel VMnFeCoNi alloy is investigated, alongside the estimation of the grain size effect on hardness. Analysis of a wide grain size range of recrystallized microstructures (12–210 µm) reveals a low annealing twin density.
Aditya Srinivasan Tirunilai +6 more
wiley +1 more source
Redox transformation of aqueous contaminants mediated by interfacial iron species
Iron-containing mineral surfaces are of tnterest to environmental researchers because of their prevalent presence and significant activity in mediating contaminant transformation in the natural environment and engineered treatment systems.
Li, Yue
core
Electronic spin state of ferric iron in Al-bearing perovskite in the lower mantle
We investigate the effect of pressure on the electronic spin state of ferric iron on Al-bearing MgSiO3-perovskite using first-principle computations. Ferric iron (6.25 mol%) and Al ( 6.25 mol%) substitute for Mg and Si respectively.
Price, GD +11 more
core +1 more source
Hydrogen‐Assisted Fracture of Iron‐Based Fe–Ni–Al Alloys
Principal relations and fracture mechanisms of single‐phase and precipitate‐strengthened Fe–Ni–Al alloys subjected to prior electrochemical hydrogen charging are identified. The mechanisms of hydrogen effect on strength and microhardness are discussed, including hydrogen‐induced increase in microhardness and the role of hydrogen in fracture behavior ...
Nataliya Yadzhak +3 more
wiley +1 more source
Iron oxides (inhalable fraction) : MAK Value Documentation, 2011
The German Commission for the Investigation of Health Hazards of Chemical Compounds in the Work Area has re‐evaluated iron oxides, considering all toxicity endpoints.
Hartwig, Andrea +2 more
core +2 more sources
The temperature dependence of fatigue behavior in nickel‐based superalloys is investigated through high‐resolution measurements of plastic localization. While increasing temperature reduces localization and enhances fatigue performance in René 88DT, Inconel 718 exhibits a sharp degradation at intermediate temperature due to intensified slip ...
M. Calvat +5 more
wiley +1 more source
The passivation of iron in ammoniacal solutions containing copper (II) ions
In the present study it was found that the presence of millimolar amounts of copper (II) ions in ammoniacal solutions leads to the spontaneous formation of a stable passive layer on metallic iron and iron alloys with nickel and cobalt, under conditions ...
Nikoloski, A.N., D'Aloya, A
core
An iron(III)-catalyzed protocol towards 2-sulfonyl quinolines from quinoline N-oxides and sodium sulfinates was herein illustrated. The general and direct option featured for high efficiency (up to 91% yields) and good functional compatibilities (27 ...
Delie An (831835) +5 more
core +1 more source
The chemical role of iron-bearing compounds on the dynamics of phosphorus in selected Brazilian latosols was investigated. The iron oxides were characterized in an attempt to assess their main chemical-mineralogical properties influencing the ion ...
Nilton Curi +3 more
doaj +1 more source
Do not let thermal drift and instrument artifacts deceive high‐temperature nanoindentation results. We compare classical Oliver–Pharr and automatic image recognition analyses across steels and a Ni alloy to quantify these effects. Accounting for artifacts reveals systematic softening with temperature, while Cr and Ni additions boost resistance ...